In Situ Measurements of Strains in Composite Battery Electrodes during Electrochemical Cycling

The cyclic stress in lithium-ion battery electrodes induced by repeated charge and discharge cycles causes electrode degradation and fracture, resulting in reduced battery performance and lifetime. To investigate electrode mechanics as a function of electrochemical cycling, we utilize digital image correlation (DIC) to measure the strains that develop in lithium-ion battery electrodes during lithiation and delithiation processes. A composite graphite electrode is cycled galvanostatically (with constant current) in a custom battery cell while optical images of the electrode surface are captured in situ. The strain in the electrode is computed using an in-house DIC code. On average, an unconstrained composite graphite electrode expands 1.41 % during lithiation and contracts 1.33 % during delithiation. These strain values compare favorably with predictions based on the elastic properties of the composite electrode and the expansion of graphite-lithium intercalation compounds (G-LICs). The establishment of this experimental protocol will enable future studies of the relationship between electrode mechanics and battery performance.

[1]  Dahn,et al.  Phase diagram of LixC6. , 1991, Physical review. B, Condensed matter.

[2]  Xiangyun Song,et al.  Correlationship between electrode mechanics and long-term cycling performance for graphite anode in lithium ion cells , 2012 .

[3]  M. Verbrugge,et al.  Modeling diffusion-induced stress in nanowire electrode structures , 2010 .

[4]  J. Haines,et al.  International programme on chemical safety , 1996, The Lancet.

[5]  Allan F. Bower,et al.  A finite strain model of stress, diffusion, plastic flow, and electrochemical reactions in a lithium-ion half-cell , 2011 .

[6]  Dahn,et al.  Suppression of staging in lithium-intercalated carbon by disorder in the host. , 1990, Physical review. B, Condensed matter.

[7]  Daniel P. Abraham,et al.  Real-Time Stress Measurements in Lithium-ion Battery Negative-electrodes , 2012 .

[8]  M. Wohlfahrt‐Mehrens,et al.  Ageing mechanisms in lithium-ion batteries , 2005 .

[9]  Alfons van Blaaderen,et al.  Dispersions of Rhodamine-Labeled Silica Spheres: Synthesis, Characterization, and Fluorescence Confocal Scanning Laser Microscopy , 1994 .

[10]  Kevin W. Eberman,et al.  Colossal Reversible Volume Changes in Lithium Alloys , 2001 .

[11]  John Lambros,et al.  Micro- and Nanoscale Deformation Measurement of Surface and Internal Planes via Digital Image Correlation , 2007 .

[12]  J. Barlow,et al.  Optimal stress locations in finite element models , 1976 .

[13]  P. Novák,et al.  A review of the features and analyses of the solid electrolyte interphase in Li-ion batteries , 2010 .

[14]  J. Dahn,et al.  In Situ Optical Observations of Particle Motion in Alloy Negative Electrodes for Li-Ion Batteries , 2006 .

[15]  Jing Li,et al.  Sodium Carboxymethyl Cellulose A Potential Binder for Si Negative Electrodes for Li-Ion Batteries , 2007 .

[16]  Zvi Hashin,et al.  Effective thermal expansion coefficients and specific heats of composite materials , 1970 .

[17]  Jian Yu Huang,et al.  In situ TEM electrochemistry of anode materials in lithium ion batteries , 2011 .

[18]  A. Vrij,et al.  Synthesis and characterization of colloidal dispersions of fluorescent, monodisperse silica spheres , 1992 .

[19]  Daniel P. Abraham,et al.  Stress Evolution in Composite Silicon Electrodes during Lithiation/Delithiation , 2013, 1308.3873.

[20]  Leif A. Carlsson,et al.  Micromechanical materials modeling , 1990 .

[21]  Venkat Srinivasan,et al.  In situ measurements of stress evolution in silicon thin films during electrochemical lithiation and delithiation , 2010, 1108.0647.

[22]  John Lambros,et al.  Fluorescent image correlation for nanoscale deformation measurements. , 2006, Small.

[23]  Yue Qi,et al.  Threefold Increase in the Young’s Modulus of Graphite Negative Electrode during Lithium Intercalation , 2010 .

[24]  Nancy R. Sottos,et al.  Local Strain Concentrations in a Microvascular Network , 2010 .

[25]  Stephen J. Harris,et al.  In Situ Observation of Strains during Lithiation of a Graphite Electrode , 2010 .