EFFECT OF HEAT TREATMENT ON COLOR, WEIGHT LOSS, SPECIFIC GRAVITY AND EQUILIBRIUM MOISTURE CONTENT OF TWO LOW MARKET VALUED TROPICAL WOODS

Cedrelinga catenaeformis) and cedro-marinheiro (Guarea trichilioides) woods. Heat treatments caused weight loss, darkening, and decreased EMC, as the maximum temperature increased. However, no changes in specific gravity were observed as a function of heating. Cedro-marinheiro has presented the highest changes in color and weight as a function of heating, while cedroarana has shown the highest reduction in EMC. Heat treatments improved some wood properties, being a good approach to improve low market valued tropical woods. Results also suggest that resilience to reduction of hygroscopicity after heating might be related to wood specific gravity.

[1]  D. Aydemir,et al.  The influence of mass loss on the mechanical properties of heat-treated black pine wood. , 2009 .

[2]  D. Johansson Heat treatment of solid wood : effects on absorption, strength and colour , 2008 .

[3]  H. Pereira,et al.  Heat-induced colour changes of pine (Pinus pinaster) and eucalypt (Eucalyptus globulus) wood , 2008, Wood Science and Technology.

[4]  S. Chow,et al.  Thermal Softening and Degradation of Wood and Bark , 2007 .

[5]  S. Poncsák,et al.  Thermogravimetric study of high temperature treatment of aspen: effect of treatment parameters on weight loss and mechanical properties , 2007 .

[6]  Engin Derya Gezer,et al.  Mechanical and chemical behavior of spruce wood modified by heat , 2006 .

[7]  Kj Krzysztof Ptasinski,et al.  Torrefaction of wood: Part 1. Weight loss kinetics , 2006 .

[8]  Mohamed Bouazara,et al.  Effect of high temperature treatment on the mechanical properties of birch (Betula papyrifera) , 2006, Wood Science and Technology.

[9]  José Nivaldo Garcia,et al.  Densidade básica e retratibilidade da madeira de Eucalyptus grandis,submetida a diferentes temperaturas de termorretificação , 2006 .

[10]  P. Viitaniemi,et al.  The water absorption of sapwood and heartwood of Scots pine and Norway spruce heat-treated at 170 °C, 190 °C, 210 °C and 230 °C , 2006, Holz als Roh- und Werkstoff.

[11]  T. Morén,et al.  The potential of colour measurement for strength prediction of thermally treated wood , 2006, Holz als Roh- und Werkstoff.

[12]  J. Bourgois,et al.  Characterization and analysis of torrefied wood , 1988, Wood Science and Technology.

[13]  B. Sundqvist Colour changes and acid formation in wood during heating , 2004 .

[14]  P. Bekhta,et al.  Effect of High Temperature on the Change in Color, Dimensional Stability and Mechanical Properties of Spruce Wood , 2003 .

[15]  M. Sehlstedt-Persson Colour responses to heat-treatment of extractives and sap from pine and spruce , 2003 .

[16]  K. Mitsui,et al.  Changes in the Properties of Light-Irradiated Wood with Heat Treatment. Part 1. Effect of Treatment Conditions on the Change in Color , 2001 .

[17]  P. Viitaniemi,et al.  The effect of heat treatment on the properties of spruce. A preliminary report , 1994 .

[18]  A. Galvão,et al.  Secagem racional da madeira , 1985 .

[19]  Jerrold E. Winandy,et al.  The chemistry of wood strength , 2012 .

[20]  Roger M. Rowell,et al.  The Chemistry of solid wood , 1984 .

[21]  Edmund Frederick Rasmussen,et al.  Dry kiln : operator's manual , 1961 .