Synthesis WSi2 coating on W substrate by HDS method with various deposition times

[1]  G. Qiao,et al.  Robust TiN nanoparticles polysulfide anchor for Li–S storage and diffusion pathways using first principle calculations , 2020 .

[2]  A. Iqbal,et al.  Novel gravel-like NiMoO4 nanoparticles on carbon cloth for outstanding supercapacitor applications , 2020 .

[3]  Jie Wang,et al.  Effect of hot dip silicon-plating temperature on microstructure characteristics of silicide coating on tungsten substrate , 2020 .

[4]  C. Jing,et al.  The structure, mechanical and electronic properties of WSi2 from first-principles investigations , 2019, Vacuum.

[5]  Jinghui Li,et al.  Effect of hot-dip siliconizing time on phase composition and microstructure of Mo–MoSi2 high temperature structural materials , 2019, Ceramics International.

[6]  Aurangzeb,et al.  Gamma-ray shielding characteristics of flexible silicone tungsten composites. , 2019, Applied radiation and isotopes : including data, instrumentation and methods for use in agriculture, industry and medicine.

[7]  Shizhong Wei,et al.  Fabrication and mechanical properties of tungsten alloys reinforced with c-ZrO2 particles , 2018, Journal of Alloys and Compounds.

[8]  Liang Zheng,et al.  An overview of oxidation-resistant tungsten alloys for nuclear fusion , 2018, Journal of Alloys and Compounds.

[9]  Yun-gang Li,et al.  Effect of siliconizing temperature on microstructure and phase constitution of Mo–MoSi2 functionally graded materials , 2018, Ceramics International.

[10]  Yuanhua Lin,et al.  First-principles study of the effect of Cr and Al on the oxidation resistance of WSi2 , 2018 .

[11]  Yun-gang Li,et al.  Microstructure and oxidation behavior of Si–MoSi2 functionally graded coating on Mo substrate , 2017 .

[12]  Liping Huang,et al.  Microstructure characteristics and oxidation behavior of vacuum plasma sprayed tungsten disilicide coating , 2016 .

[13]  B. He,et al.  Preparation and thermal shock characterization of yttrium doped tungsten-potassium alloy , 2016 .

[14]  S. Akintunde,et al.  Kinetics of growth of thin-films of Co2Si, Ni2Si, WSi2 and VSi2 during a reactive diffusion process , 2016 .

[15]  J. Brinkmann,et al.  Development of yttrium-containing self-passivating tungsten alloys for future fusion power plant , 2016 .

[16]  M. Shamanian,et al.  Evaluation of oxidation behavior of laser clad CoWSi–WSi2 coating on pure Ni substrate at different temperatures , 2015 .

[17]  F. Zheng,et al.  Thermal Shock and Ablation Behavior of Tungsten Nozzle Produced by Plasma Spray Forming and Hot Isostatic Pressing , 2015, Journal of Thermal Spray Technology.

[18]  Ch. Linsmeier,et al.  Oxidation behaviour of silicon-free tungsten alloys for use as the first wall material , 2011 .

[19]  Yujun Shi,et al.  Effect of filament temperature and deposition time on the formation of tungsten silicide with silane , 2011 .

[20]  D. Das,et al.  Formation of WSi2 coating on tungsten and its short-term cyclic oxidation performance in air , 2011 .

[21]  J. Puszynski,et al.  Synthesis of WSi2 -SiC composite under the thermally activated combustion mode , 2010 .

[22]  Sung-Jae Chung,et al.  Growth kinetics and oxidation behavior of WSi2 coating formed by chemical vapor deposition of Si on W substrate , 2006 .

[23]  R. Mitra Mechanical behaviour and oxidation resistance of structural silicides , 2006 .

[24]  L. Čížek,et al.  Structure and mechanical properties of formed tungsten based materials , 2004 .

[25]  W. Yoon,et al.  Growth kinetics of W5Si3 layer in WSi2/W system , 2004 .

[26]  B. Sell,et al.  Chemical vapor deposition of tungsten silicide (WSix) for high aspect ratio applications , 2003 .

[27]  J. Yao,et al.  Simulation of the sublimation process in the preparation of photochromic WO3 film by laser microprobe mass spectrometry , 2000 .

[28]  P. J. Meschter Low-temperature oxidation of molybdenum disilicide , 1992 .

[29]  E. A. Gulbransen Thermochemistry and the Oxidation of Refractory Metals at High Temperature , 1970 .

[30]  J. H. Westbrook,et al.  “PEST” degradation in beryllides, silicides, aluminides, and related compounds , 1964 .

[31]  S. N. Goldstein,et al.  Mass‐Spectrometric Investigation of the Oxidation of Molybdenum and Tungsten , 1963 .

[32]  E. A. Gulbransen,et al.  Kinetics of the Oxidation of Pure Tungsten from 500° to 1300°C , 1960 .