The thermal and mechanical properties of a new negative photoresist, SU8, were characterized. The influence of curing conditions, such as baking temperature, baking time and UV dosage, on the thermal and mechanical properties of the resultant coatings was studied in detail. It was found that the glass-transition temperature (Tg) of the coatings was coincident with the baking temperature over the temperature range of 25 °C–220 °C for coatings being baked for just 20 min. However, the Tg reached a limiting value (about 240 °C) once the cross-linking reaction was complete, and would not increase further with the baking temperature. The peak temperature of the dimension versus temperature plots, where heat shrinkage occurred, was about a factor of 1.16 times higher than the baking temperature for the temperature range studied. Both the Tg and the shrinkage temperature were affected by the baking time. The thermal expansion coefficients (TEC), including the volumetric TEC (αv), the in-plane TEC (α1) and the out-of-plane TEC (α2), were measured by a pressure–volume–temperature (PVT) apparatus and thermal–mechanical analyzer (TMA). Great residual stress could be generated during the process, and the change in residual stress with the environmental humidity was investigated using vibrational holographic interferometry.
[1]
M. Maden.
The determination of stresses and material properties of polyimide coatings and films using real time holographic interferometry
,
1992
.
[2]
R. Farris,et al.
Vibrational Technique for Stress Measurement in Films: I, Ideal Membrane Behavior
,
1994
.
[3]
Jane M. Shaw,et al.
Micromachining applications of a high resolution ultrathick photoresist
,
1995
.
[4]
M. Despont,et al.
SU-8: a low-cost negative resist for MEMS
,
1997
.
[5]
Steven J. Holmes,et al.
Negative photoresists for optical lithography
,
1997,
IBM J. Res. Dev..
[6]
M. Laudon,et al.
Mechanical characterization of a new high-aspect-ratio near UV-photoresist
,
1998
.