Microstructure and ablation performance of SiC–ZrC coated C/C composites prepared by reactive melt infiltration
暂无分享,去创建一个
Yicheng Ge | Zhe Zhou | Liping Ran | Ke Peng | Zexu Sun | M. Yi
[1] Jiabao Zhang,et al. Microstructure and ablation mechanism of C/C-ZrC-SiC composites in a plasma flame , 2017 .
[2] Hejun Li,et al. Ablation resistance of supersonic-atmosphere-plasma-spraying ZrC coating doped with ZrO2 for SiC-coated carbon/carbon composites , 2017 .
[3] J. Ouyang,et al. Effect of deposition time on growth of ZrC/SiC composite coating synthesized by low pressure chemical vapor deposition , 2017 .
[4] Kezhi Li,et al. HfC-ZrC-SiC multiphase protective coating for SiC-coated C/C composites prepared by supersonic atmospheric plasma spraying , 2017 .
[5] Kezhi Li,et al. Directional thermophysical, ablative and compressive behavior of 3D carbon/carbon composites , 2015 .
[6] Hejun Li,et al. Effect of pre-oxidation treatment on the bonding strength and thermal shock resistance of SiC coating for C/C–ZrC–SiC composites , 2015 .
[7] Xiaohong Shi,et al. Ablation resistance of SiC–ZrC coating prepared by a simple two-step method on carbon fiber reinforced composites , 2014 .
[8] B. Wen,et al. Supersonic flame ablation resistance of W/ZrC coating deposited on C/SiC composites by atmosphere plasma spraying , 2014 .
[9] Wen Jie Chen,et al. Thermodynamic Assessment of SiO2-ZrO2 Binary System , 2014 .
[10] Jianfeng Huang,et al. A mullite/SiC oxidation protective coating for carbon/carbon composites , 2013 .
[11] Hejun Li,et al. Preparation and ablation properties of ZrC-SiC coating for carbon/carbon composites by solid phase infiltration , 2011 .
[12] Hejun Li,et al. Microstructures and Ablation Resistance of ZrC Coating for SiC-Coated Carbon/Carbon Composites Prepared by Supersonic Plasma Spraying , 2011 .
[13] Lai-fei Cheng,et al. Laser ablation behaviors of SiC–ZrC coated carbon/carbon composites , 2011 .
[14] Hejun Li,et al. Ablation of the carbon/carbon composite nozzle-throats in a small solid rocket motor , 2011 .
[15] William E Lee,et al. Reactive infiltration processing (RIP) of ultra high temperature ceramics (UHTC) into porous C/C composite tubes , 2011 .
[16] Hejun Li,et al. Ablative property of HfC-based multilayer coating for C/C composites under oxy-acetylene torch , 2011 .
[17] Li Guodong,et al. Texture structure and ablation behavior of TaC coating on carbon/carbon composites , 2010 .
[18] Qizhong Huang,et al. Preparation of ZrC-SiC Multi-coating on Graphite with ZrSiO 4 Powder via Pack Cementation: Preparation of ZrC-SiC Multi-coating on Graphite with ZrSiO 4 Powder via Pack Cementation , 2009 .
[19] Wei Sun,et al. ZrC ablation protective coating for carbon/carbon composites , 2009 .
[20] Jong Hoon Park,et al. Temperature dependency of the LPCVD growth of ZrC with the ZrCl4–CH4–H2 system , 2008 .
[21] H. Joo,et al. Ablation characteristics of carbon fiber reinforced carbon (CFRC) composites in the presence of silicon carbide (SiC) coating , 2004 .
[22] Q. Guo,et al. Resistance to ablation of pitch-derived ZrC/C composites , 2004 .
[23] G. Blount,et al. Carbon-carbon composites: a summary of recent developments and applications , 1997 .
[24] Richard J. Day,et al. Oxidation protection for carbon fibre composites , 1996, Journal of Materials Science.
[25] T. I. Barry,et al. The calculation of phase equilibria of oxide core-concrete systems , 1993 .