Age-hardening characteristics in an AuCu-14at.%Ag alloy
暂无分享,去创建一个
[1] G. Tendeloo,et al. Microstructure of AuCu II in the disordered f.c.c. phase of AuCu-14at.%Ag alloy , 1991 .
[2] M. Nakagawa,et al. A coherent phase diagram of the Aux(Ag0.24Cu0.76)1−x section of the AuCuAg ternary system , 1988 .
[3] S. Amelinckx,et al. High-resolution Electron Microscopic Study of Age-hardening in a Commercial Dental Gold Alloy , 1986, Journal of dental research.
[4] K. Yasuda,et al. Age-hardening characteristics in an 18 carat gold commercial dental alloy containing palladium , 1986 .
[5] K. Hisatsune,et al. Isothermal age-hardening behaviour in commercial dental gold alloys containing palladium. , 1984, Dental materials journal.
[6] K. Yasuda,et al. Age-hardening mechanism of equiatomic AuCu and AuCu-Ag pseudo-binary alloys. , 1983, Dental materials journal.
[7] K. Hisatsune,et al. Structural changes induced by ageing in commercial dental gold alloys containing palladium. , 1983, Dental materials journal.
[8] K. Yasuda,et al. Difference in Age-hardening Mechanism in Dental Gold Alloys , 1982, Journal of dental research.
[9] K. Hisatsune,et al. Age hardening in a dental white gold alloy , 1982 .
[10] K. Yasuda,et al. Determination of the AuCu Superlattice Formation Region in Gold-Copper-Silver Ternary System , 1981, Journal of dental research.
[11] K. Yasuda,et al. Age-hardening characteristics of a commercial dental gold alloy☆ , 1980 .
[12] K. Yasuda,et al. Structure and morphology of an age-hardened goldcopper-silver dental alloy , 1978 .
[13] K. Yasuda,et al. Structural changes caused by age-hardening in a dental gold alloy , 1975 .
[14] S. Mizuno,et al. A Theoretical Analysis of the Phase-Decompositions Based upon the Non-Linear Diffusion Equation , 1983 .
[15] J. Linde. Röntgenographische und elektrische Untersuchungen des CuAu-Systems , 1936 .