Dielectric breakdown in silica-amorphous polymer nanocomposite films: the role of the polymer matrix.

The ultimate energy storage performance of an electrostatic capacitor is determined by the dielectric characteristics of the material separating its conductive electrodes. Polymers are commonly employed due to their processability and high breakdown strength; however, demands for higher energy storage have encouraged investigations of ceramic-polymer composites. Maintaining dielectric strength, and thus minimizing flaw size and heterogeneities, has focused development toward nanocomposite (NC) films; but results lack consistency, potentially due to variations in polymer purity, nanoparticle surface treatments, nanoparticle size, and film morphology. To experimentally establish the dominant factors in broad structure-performance relationships, we compare the dielectric properties for four high-purity amorphous polymer films (polymethyl methacrylate, polystyrene, polyimide, and poly-4-vinylpyridine) incorporating uniformly dispersed silica colloids (up to 45% v/v). Factors known to contribute to premature breakdown-field exclusion and agglomeration-have been mitigated in this experiment to focus on what impact the polymer and polymer-nanoparticle interactions have on breakdown. Our findings indicate that adding colloidal silica to higher breakdown strength amorphous polymers (polymethyl methacrylate and polyimide) causes a reduction in dielectric strength as compared to the neat polymer. Alternatively, low breakdown strength amorphous polymers (poly-4-vinylpyridine and especially polystyrene) with comparable silica dispersion show similar or even improved breakdown strength for 7.5-15% v/v silica. At ∼15% v/v or greater silica content, all the polymer NC films exhibit breakdown at similar electric fields, implying that at these loadings failure becomes independent of polymer matrix and is dominated by silica.

[1]  F. Doğan,et al.  Improved polymer nanocomposite dielectric breakdown performance through barium titanate to epoxy interface control , 2011 .

[2]  Hilmar Koerner,et al.  Nanolaminates: increasing dielectric breakdown strength of composites. , 2012, ACS applied materials & interfaces.

[3]  Stephen Ducharme,et al.  Electric energy density of dielectric nanocomposites , 2007 .

[4]  T. Schutte,et al.  DC breakdown strength of polypropylene films: area dependence and statistical behavior , 2007, IEEE Transactions on Dielectrics and Electrical Insulation.

[5]  A. Hiltner,et al.  Imaging the effect of dielectric breakdown in a multilayered polymer film , 2012 .

[6]  Harvey Scher,et al.  Critical Density in Percolation Processes , 1970 .

[7]  R. Vaia,et al.  Breakdown Voltage of Thermoplastics with Clay Nanometer-Sized Fillers , 2008, 2008 IEEE International Power Modulators and High-Voltage Conference.

[8]  J. Calame Finite difference simulations of permittivity and electric field statistics in ceramic-polymer composites for capacitor applications , 2006 .

[9]  Percolation model for electrical breakdown in insulating polymers , 2004 .

[10]  E. Tuncer,et al.  Enhancement of dielectric strength in nanocomposites , 2007 .

[11]  J. K. Nelson,et al.  Dielectric Polymer Nanocomposites , 2010 .

[12]  M. Pettersson,et al.  Dielectric properties and partial discharge endurance of polypropylene-silica nanocomposite , 2010, IEEE Transactions on Dielectrics and Electrical Insulation.

[13]  S. Ducharme An inside-out approach to storing electrostatic energy. , 2009, ACS nano.

[14]  Clive A. Randall,et al.  High field properties and energy storage in nanocomposite dielectrics of poly(vinylidene fluoride-hexafluoropropylene) , 2011 .

[15]  Lei Zhu,et al.  Polymer nanocomposites for electrical energy storage , 2011 .

[16]  Ming-Jen Pan,et al.  High energy density nanocomposites based on surface-modified BaTiO(3) and a ferroelectric polymer. , 2009, ACS nano.

[17]  H. Ploehn,et al.  Polymer Composite and Nanocomposite Dielectric Materials for Pulse Power Energy Storage † , 2009, Materials.

[18]  A. Hiltner,et al.  Enhanced breakdown strength of multilayered films fabricated by forced assembly microlayer coextrusion , 2009 .

[19]  S. Weigand,et al.  Development of Filler Structure in Colloidal Silica–Polymer Nanocomposites , 2011 .

[20]  C. Randall,et al.  Polyethylene nanocomposite dielectrics: Implications of nanofiller orientation on high field properties and energy storage , 2011 .

[21]  J. Won,et al.  Barium Titanate Nanoparticles with Diblock Copolymer Shielding Layers for High-Energy Density Nanocomposites , 2010 .

[22]  L. Schadler,et al.  Polymer nanocomposite dielectrics-the role of the interface , 2005, IEEE Transactions on Dielectrics and Electrical Insulation.

[23]  T. Lewis Interfaces are the dominant feature of dielectrics at the nanometric level , 2004, IEEE Transactions on Dielectrics and Electrical Insulation.

[24]  J. Fothergill,et al.  Internal charge behaviour of nanocomposites , 2004 .

[25]  R. Vogelsang,et al.  The effect of barriers on electrical tree propagation in composite insulation materials , 2006, IEEE Transactions on Dielectrics and Electrical Insulation.

[26]  K. Younsi,et al.  The future of nanodielectrics in the electrical power industry , 2004, IEEE Transactions on Dielectrics and Electrical Insulation.

[27]  G. Kofod,et al.  Increased permittivity nanocomposite dielectrics by controlled interfacial interactions , 2012 .

[28]  Shengtao Li,et al.  Fabrication and Dielectric Characterization of Advanced BaTiO3/Polyimide Nanocomposite Films with High Thermal Stability , 2008 .

[29]  Lisa A. Fredin,et al.  Enhanced Energy Storage and Suppressed Dielectric Loss in Oxide Core–Shell–Polyolefin Nanocomposites by Moderating Internal Surface Area and Increasing Shell Thickness , 2012, Advanced materials.

[30]  J. K. Nelson,et al.  Candidate mechanisms controlling the electrical characteristics of silica/XLPE nanodielectrics , 2007 .