Tensile deformation and fracture behavior of spray-deposition 7075/15SiCp aluminum matrix composite sheet at elevated temperatures

[1]  Hui Zhang,et al.  Dynamic and static softening behaviors of aluminum alloys during multistage hot deformation , 2004 .

[2]  W. Kim,et al.  Particle weakening in superplastic SiC/2124 Al composites at high temperature , 2000 .

[3]  M. Mabuchi,et al.  The role of partial melting on superplasticity of Si3N4p/Al-Cu-Mg composite , 2000 .

[4]  K. Chan,et al.  Deformation behavior of a PM Al6013/15SiCP composite sheet at elevated temperature , 1999 .

[5]  Keith C. C. Chan,et al.  Hot formability of an Al2009/20SiCW composite sheet , 1998 .

[6]  Y. Chen,et al.  Superplastic deformation of SiCp/2024 Al composite fabricated by spray atomization and codeposition , 1997 .

[7]  A. Jackson,et al.  Constitutive equations for use in prediction of flow stress during extrusion of aluminium alloys , 1997 .

[8]  T. Yue,et al.  Constitutive equations for superplastic deformation of SiC particulate reinforced aluminum alloys , 1996 .

[9]  E. Cerri,et al.  Comparative hot workability of 7012 and 7075 alloys after different pretreatments , 1995 .

[10]  Y. Nishida,et al.  High strain rate superplasticity of Si3N4 whisker reinforced 7075 alloy matrix composite fabricated by squeeze casting , 1995 .

[11]  T. Nieh,et al.  Superplasticity at high strain rates in a SiC Whisker reinforced A1 alloy , 1984 .

[12]  A. Razaghian,et al.  Fracture behaviour of a SiC-particle-reinforced aluminium alloy at high temperature , 1998 .

[13]  W. Lau,et al.  High temperature deformation behavior of Al 2124-SiCp composite , 1997 .