Interdental design of porcelain veneers in the presence of composite fillings: finite element analysis of composite shrinkage and thermal stresses.

PURPOSE This study was conducted to optimize the interdental design (wraparound) of porcelain laminates bonded to teeth in the presence of preexisting composite fillings. MATERIALS AND METHODS A finite element model (2-dimensional mesh generated from a horizontal cross section of a maxillary incisor) was used to evaluate the effects of luting composite shrinkage and thermal changes on the stress distribution within the ceramic. The mesh included 3 restorative designs (3 degrees of interdental wrapping) and a Class III composite filling. Curing contraction of the luting composite was simulated at baseline temperature (37 degrees C). Thermal loads from 37 to 60 degrees C and from 37 to 5 degrees C were assessed with and without preexisting composite shrinkage. Surface tangential stresses were calculated at the ceramic surface and interface. RESULTS Curing contraction alone generated mostly compressive stresses (peaks at 15 MPa) at both the ceramic surface and interface. Stresses remained compressive (peaks at 20 MPa) when thermal changes were added, except for the conservative veneer with minimum wraparound, the margins of which showed potentially harmful tensile stress peaks (approximately 7 MPa). Deformation of the tooth-restoration complex tended to be more uniform for veneers with maximum wraparound. In the presence of thermal loads alone, opposite effects were observed on the restoration surface and the interface, with compressive stresses on one side (up to 13 MPa) and tensile stresses on the other (up to 9 MPa). This effect of proximal bending (explained by the nearby expansion/contraction of the composite filling) was attenuated by the significant reduction of the bulk of the preexisting interdental composite by the overlapping veneer. CONCLUSION In the finite element environment, the negative effect of the nearby expanding/contracting composite fillings can be minimized by extending the veneer over the preexisting interdental restoration. Because of the precompressed state resulting from composite shrinkage, ceramics showed lower temperature-induced tensile stresses.

[1]  E. Munksgaard,et al.  Reinforcement of bonded crown fractured incisors with porcelain veneers. , 1991, Endodontics & dental traumatology.

[2]  W. Douglas,et al.  Additive contour of porcelain veneers: a key element in enamel preservation, adhesion, and esthetics for aging dentition. , 1999, The journal of adhesive dentistry.

[3]  M. Fradeani Six-year follow-up with Empress veneers. , 1998, The International journal of periodontics & restorative dentistry.

[4]  A. Caputo,et al.  A photoelastic study of stresses on porcelain laminate preparations. , 1987, The Journal of prosthetic dentistry.

[5]  E. Munksgaard,et al.  Treatment of crown fractured incisors with laminate veneer restorations. An experimental study. , 1992, Endodontics & dental traumatology.

[6]  James M. Gere,et al.  Analysis of Stress and Strain , 1991 .

[7]  E. K. Hansen,et al.  Marginal adaptation of posterior resins: effect of dentin-bonding agent and hygroscopic expansion. , 1989, Dental materials : official publication of the Academy of Dental Materials.

[8]  A. Walls The use of adhesively retained all-porcelain veneers during the management of fractured and worn anterior teeth: Part 1. Clinical technique , 1995, British Dental Journal.

[9]  T. Wang,et al.  Measurement of thermal expansion coefficient of human teeth. , 1990, Australian dental journal.

[10]  A. Plasschaert,et al.  Failure Stress Criteria for Composite Resin , 1987, Journal of dental research.

[11]  T W Korioth,et al.  Modeling the mechanical behavior of the jaws and their related structures by finite element (FE) analysis. , 1997, Critical reviews in oral biology and medicine : an official publication of the American Association of Oral Biologists.

[12]  Wang Tong,et al.  Measurement of thermal expansion coefficient of human teeth , 1989 .

[13]  U. Belser,et al.  Natural and restorative oral esthetics. Part II: Esthetic treatment modalities. , 1993, Journal of esthetic dentistry.

[14]  N. Creugers,et al.  patients' satisfaction with different types of veneer restorations. , 1997, Journal of dentistry.

[15]  L. G. Davis,et al.  The effect of porcelain laminate veneers on gingival health and bacterial plaque characteristics. , 1994, Journal of clinical periodontology.

[16]  K. Itoh,et al.  Effect of water sorption and thermal stress on cavity adaptation of dental composites. , 1990, Dental materials : official publication of the Academy of Dental Materials.

[17]  P Magne,et al.  Porcelain veneers: dentin bonding optimization and biomimetic recovery of the crown. , 1999, The International journal of prosthodontics.

[18]  W. Douglas,et al.  Cumulative effects of successive restorative procedures on anterior crown flexure: intact versus veneered incisors. , 2014, Quintessence International.

[19]  R DeLong,et al.  Biophysical stress analysis of restored teeth: modelling and analysis. , 1988, Dental materials : official publication of the Academy of Dental Materials.

[20]  J S Rouse,et al.  Full veneer versus traditional veneer preparation: a discussion of interproximal extension. , 1997, The Journal of prosthetic dentistry.

[21]  A. Versluis,et al.  Thermal expansion coefficient of dental composites measured with strain gauges. , 1996, Dental materials : official publication of the Academy of Dental Materials.

[22]  J. Sorensen,et al.  Marginal fidelity and microleakage of porcelain veneers made by two techniques. , 1992, The Journal of prosthetic dentistry.

[23]  P Magne,et al.  Effect of luting composite shrinkage and thermal loads on the stress distribution in porcelain laminate veneers. , 1999, The Journal of prosthetic dentistry.

[24]  T. Berry,et al.  Post-bonding crack formation in porcelain veneers. , 1997, Journal of esthetic dentistry.

[25]  R. Jacobi,et al.  The ceramic reverse three-quarter crown for anterior teeth: preparation design. , 1989, The Journal of prosthetic dentistry.

[26]  A W Walls,et al.  The use of adhesively retained all-porcelain veneers during the management of fractured and worn anterior teeth: Part 2. Clinical results after 5 years of follow-up , 1995, British Dental Journal.

[27]  R DeLong,et al.  Biophysical stress analysis of restored teeth: experimental strain measurement. , 1988, Dental materials : official publication of the Academy of Dental Materials.

[28]  J. Hodges,et al.  Crack propensity of porcelain laminate veneers: A simulated operatory evaluation. , 1999, The Journal of prosthetic dentistry.

[29]  D. Watts,et al.  Temperature-dependence of Compressive Properties of Human Dentin , 1987, Journal of dental research.

[30]  Z. Li,et al.  Cyclic mechanical fatigue of a feldspathic dental porcelain. , 1995, The International journal of prosthodontics.

[31]  J. Calamia Clinical evaluation of etched porcelain veneers. , 1989, American journal of dentistry.

[32]  K J Anusavice,et al.  Influence of Incisal Length of Ceramic and Loading Orientation on Stress Distribution in Ceramic Crowns , 1988, Journal of dental research.

[33]  D. N. Misra,et al.  Sorption of Water by Filled-Resin Composites , 1977, Journal of dental research.

[34]  M. Barco,et al.  Temperature extremes produced orally by hot and cold liquids. , 1992, The Journal of prosthetic dentistry.

[35]  P Magne,et al.  Ceramic laminate veneers: continuous evolution of indications. , 1997, Journal of esthetic dentistry.

[36]  C. Davidson,et al.  Relaxation of Polymerization Contraction Shear Stress by Hygroscopic Expansion , 1990, Journal of dental research.