THE INTRINSIC DEGRADATION PHENOMENA OF LANI5 AND LANI4.7AL0.3 BY TEMPERATURE INDUCED HYDROGEN ABSORPTION-DESORPTION CYCLING

[1]  K. N. Semenenko,et al.  Physicochemistry and crystallochemistry of intermetallic hydrides containing rare earths and transition metals , 1985 .

[2]  S. Suda Experimental evaluation of heat pump performance in connection with metal hydride properties , 1984 .

[3]  M. Ron,et al.  A hydrogen heat pump as a bus air conditioner , 1984 .

[4]  H. Uchida,et al.  Effect of the pulverization of LaNi5 on the hydrogen absorption rate and the X-ray diffraction patterns , 1984 .

[5]  P. D. Goodell,et al.  Stability of rechargeable hydriding alloys during extended cycling , 1984 .

[6]  P. Rudman,et al.  Hydriding and dehydriding kinetics , 1983 .

[7]  K. Buschow Intermetallic compounds, amorphous alloys and ternary hydrides based on rare earth elements , 1982 .

[8]  Jai-Young Lee,et al.  A study on the kinetics of hydriding of the LaNi5 system , 1982 .

[9]  T. Flanagan,et al.  The effect of annealing on plateau hydrogen pressures and hysteresis in the LaNi5H system , 1981 .

[10]  D. Gruen,et al.  Temperature-programmed desorption (TPD) studies of ZrV1.6Fe0.4Hy and ZrV1.2Cr0.8Hy , 1981 .

[11]  R. L. Cohen,et al.  Degradation of LaNi5 by temperature-induced cycling , 1980 .

[12]  L. Schlapbach,et al.  Surface effects and the formation of metal hydrides , 1980 .

[13]  J. H. Wernick,et al.  Degradation of Lani5 hydrogen-absorbing material by cycling , 1980 .

[14]  R. L. Cohen,et al.  Degradation of hydrogen-absorbing rare earth intermetallics by cycling , 1978 .

[15]  A. Maeland,et al.  Hydrides of lanthanum-nickel compounds , 1976 .

[16]  K. Buschow,et al.  Phase relations and hydrogen absorption in the lanthanum-nickel system , 1972 .

[17]  E. M. Sherwood Less Common Metals , 1956 .