Crack-initiation toughness and crack-arrest toughness in advanced 9 pct Ni steel welds containing local brittle zones

[1]  Fumiyoshi Minami,et al.  Effect of Strength Mis-Match on Fracture Mechanical Behavior of HAZ-Notched Weld Joint , 1995 .

[2]  M. Toyoda,et al.  Study on Micro-crack Initiation Properties in Stell HAZ having Microscopical Heterogeneity in Strength. (Report 2). Property Distribution Map to understand HAZ CTOD Toughness. , 1995 .

[3]  Julia King,et al.  Cleavage initiation in the intercritically reheated coarse-grained heat-affected zone: Part I. Fractographic evidence , 1994 .

[4]  D. Kwon,et al.  Correlation of microstructure and fracture properties in weld heat- affected zones of thermomechanically controlled processed steels , 1992 .

[5]  John M. Potter,et al.  Fatigue and Fracture Testing of Weldments , 1990 .

[6]  Y. Nakao,et al.  Distribution of Toughness in HAZ of Multi-Pass Welded High Strength Steel : Study on Distribution of Microstructure and Toughness in Multi-Pass Weld HAZ (Report 2) , 1985 .

[7]  K. Masubuchi Analysis of Welded Structures , 1980 .

[8]  A. Götte,et al.  Metall , 1897 .

[9]  K. Ray,et al.  Fracture criteria of deep-drawn steel sheets , 1994 .

[10]  M. Toyoda Brittle Fracture Strength and Fracture Toughness Evaluation of Welds. Significance of Welding Mechanics Researches on Fracture Integrity of Welds. , 1993 .

[11]  D. Y. Lee,et al.  Microstructure and local brittle zone phenomena in high-strength low-alloy steel welds , 1991 .

[12]  D. Fairchild Fracture Toughness Testing of Weld Heat-Affected Zones in Structural Steel , 1990 .

[13]  C. Syn,et al.  Microstructural sources of toughness in QLT-Treated 5.5Ni cryogenic steel , 1983 .