Size and shape evolution of faceted bicrystal nanoparticles of gold on sapphire

Abstract We produced an array of Au nanoparticles on the basal plane of sapphire via solid-state dewetting of a thin film, and followed the size and shape evolution of individual particles during a 950 °C anneal in air. The particles exhibited {1 0 0} and {1 1 1} facets and shapes that tend to be far from those predicted based upon equilibrium considerations. Most of the single-crystal particles exhibited remarkable size and shape stability up to the longest annealing time, 65 h. The bicrystal particles rapidly transformed into single crystals after the shortest annealing time, 1 h. This transformation was accompanied by an apparent rotation of one of the grains and its alignment along its immobile counterpart. We interpreted both phenomena in terms of very slow mass transport along the singular {1 1 1} and {1 0 0} facets. In the case of bicrystal particles, the fast migration and escape of the boundary from the particle changed the crystallography of the facets in the grain swept by the boundary from a crystallographically singular orientation to a non-special orientation. Such surfaces exhibit high diffusivity and, hence, rapid shape evolution via curvature-driven surface diffusion. A quantitative model of this rotation was proposed and showed to confirm our qualitative description. Based on these findings, we conclude that grain-boundary migration, rather than surface diffusivity, controls the kinetics of mid- and late-term agglomeration of thin polycrystalline films of Au.

[1]  W. Kaplan,et al.  Morphology and orientation of the equilibrated Au–sapphire $$ \left( {10\bar 10} \right) $$ interface , 2006 .

[2]  Rishi Raj,et al.  Copper on sapphire: Stability of thin films at 0.7 Tm , 1989 .

[3]  E. Rabkin,et al.  Scanning probe microscopy study of grain boundary migration in NiAl , 2004 .

[4]  K. Thelander A review of nanowire growth promoted by alloys and non-alloying elements with emphasis on Au-assisted III-V nanowires , 2008 .

[5]  I. Szabó,et al.  Morphological evolution of thin gold films studied by Auger electron spectroscopy in beading conditions , 2004 .

[6]  D. Srolovitz,et al.  Nanoindentation size effect in single-crystal nanoparticles and thin films: A comparative experimental and simulation study , 2011 .

[7]  Carl V. Thompson,et al.  Capillary instabilities in thin, continuous films , 1992 .

[8]  E. Rabkin,et al.  Grain boundary grooving in molybdenum bicrystals , 2006 .

[9]  H. Wong,et al.  A spike-function model of facets , 2004 .

[10]  Erwan Dornel,et al.  Surface diffusion dewetting of thin solid films: Numerical method and application to Si/SiO 2 , 2006 .

[11]  Y. Mishin,et al.  Fundamentals of grain and interphase boundary diffusion , 1995 .

[12]  P. Wynblatt,et al.  Equilibrium Shape of Copper Crystals Grown on Sapphire , 2004 .

[13]  J. Hirth,et al.  Surface self-diffusion on gold , 1968 .

[14]  R. W. Balluffi,et al.  Interfaces in crystalline materials , 2009 .

[15]  B. Cuenya Synthesis and catalytic properties of metal nanoparticles: Size, shape, support, composition, and oxidation state effects , 2010 .

[16]  E. Rabkin,et al.  Jerky motion of grain boundaries in NiAl : An atomic force microscopy study , 2000 .

[17]  W. L Winterbottom,et al.  Equilibrium shape of a small particle in contact with a foreign substrate , 1967 .

[18]  T. Seong,et al.  Effect of different metal deposition methods on the growth behaviors of carbon nanotubes , 2007 .

[19]  W. Mullins,et al.  Nucleation Barrier for Volume‐Conserving Shape Changes of Faceted Crystals , 2000 .

[20]  E. Rabkin,et al.  GRAIN BOUNDARY GROOVING AT THE SINGULAR SURFACES , 2000 .

[21]  Tae-Sik Yoon,et al.  Comparison of the agglomeration behavior of Au and Cu films sputter deposited on silicon dioxide , 2003 .

[22]  W. Kaplan,et al.  Au–Sapphire (0001) solid–solid interfacial energy , 2006 .

[23]  Ralph Spolenak,et al.  Microstructure evolution during dewetting in thin Au films , 2010 .