Effect of Cr and Mn on the microstructure of spray-formed Al–25Si–5Fe–3Cu alloy

[1]  L. Hou,et al.  Effect of (Mn + Cr) addition on the microstructure and thermal stability of spray-formed hypereutectic Al–Si alloys , 2009 .

[2]  W. Eidhed Modification of β-Al5FeSi Compound in Recycled Al-Si-Fe Cast Alloy by Using Sr, Mg and Cr Additions , 2009 .

[3]  B. Xiong,et al.  Effect of Fe and Mn additions on microstructure and mechanical properties of spray-deposited Al–20Si–3Cu–1 Mg alloy , 2009 .

[4]  Haiyou Huang,et al.  Influence of Mn addition on microstructure and phase formation of spray-deposited Al–25Si–xFe–yMn alloy , 2009 .

[5]  A. Simchi,et al.  Effect of particle size on the microstructure of rapidly solidified Al–20Si–5Fe–2X (X = Cu, Ni, Cr) powder , 2008 .

[6]  A. Simchi,et al.  Microstructure and mechanical properties of Al–20Si–5Fe–2X (X = Cu, Ni, Cr) alloys produced by melt-spinning , 2008 .

[7]  D. H. Wang,et al.  Soft magnetic properties and microstructure of novel Nb poor Finemet type alloys , 2008 .

[8]  F. Samuel,et al.  Effect of metallurgical parameters on the hardness and microstructural characterization of as-cast and heat-treated 356 and 319 aluminum alloys , 2007 .

[9]  Hyuck-Mo Lee,et al.  The influence of Mn and Cr on the tensile properties of A356–0.20Fe alloy , 2006 .

[10]  A. Srivastava,et al.  Microstructural features induced by spray processing and hot extrusion of an Al–18% Si–5% Fe–1.5% Cu alloy , 2006 .

[11]  C. Tsao,et al.  Microstructures and mechanical properties of spray-formed and squeeze-cast Al–25Si–0.89Cu–1.0Ni–0.84Mg alloys in solutionized and aged conditions , 2006 .

[12]  D. Eskin,et al.  Constituent phase diagrams of the Al–Cu–Fe–Mg–Ni–Si system and their application to the analysis of aluminium piston alloys , 2005 .

[13]  P. Lazar,et al.  Structural study on Al-26 mass% Si-8 mass% Ni powder , 2005 .

[14]  M. Emamy,et al.  Precipitation of Fe rich intermetallics in Cr- and Co-modified A413 alloy , 2005 .

[15]  S. Shabestari,et al.  Effect of copper and solidification conditions on the microstructure and mechanical properties of Al–Si–Mg alloys , 2004 .

[16]  H. Ye,et al.  An overview of the development of Al-Si-Alloy based material for engine applications , 2003 .

[17]  T. Mitani,et al.  A new approach to molecular devices using SAMs, LSMCD and Cat-CVD , 2003 .

[18]  P. Ghosal,et al.  Microstructure and phase formation in spray-deposited Al–18%Si–5%Fe–1.5%Cu alloy , 2002 .

[19]  B. Xiong,et al.  The effect of Mn on the microstructure of spray-deposited Al–20Si–5Fe–3Cu–1Mg alloy , 2001 .

[20]  F. Froes,et al.  Characterization investigations of melt-spun ternary Al–xSi–3.3Fe (x=10, 20 wt.%) alloys , 2001 .

[21]  L. Froyen,et al.  Solid ↔ liquid phase transformations in hypereutectic P/M Al-Si-Fe-X alloys , 2000 .

[22]  C. Suryanarayana,et al.  Effect of alloying elements and degassing pressure on the structure and mechanical properties of rapidly solidified Al–20Si–5Fe–2X (X=Cr, Zr, or Ni) alloys , 2000 .

[23]  N. Tawfik Mechanical properties of rapidly solidified ribbons of some AI–Si based alloys , 1997 .

[24]  E. Lavernia,et al.  Spray Atomization and Deposition , 1996 .

[25]  Manoj Gupta,et al.  Effect of processing on the microstructural variation and heat-treatment response of a hypercutectic AlSi alloy , 1995 .

[26]  J. Gruzleski,et al.  The Effect of Solidification Condition and Chemistry on the Formation and Morphology of Complex Intermetallic Compounds in Aluminium—Silicon Alloys , 1994 .

[27]  B. Verlinden,et al.  Characterization of the hot-working behaviour of a P/M Al-20Si-7.5Ni-3Cu-1Mg alloy by hot torsion , 1992 .

[28]  L. F. Mondolfo Aluminum alloys: Structure and properties , 1976 .