Wear behavior of Fe-Cr-B alloys under dry sliding condition

Purpose – The purpose of this study is to prepare new Fe-Cr-B alloys which have better wear resistance and investigate the wear mechanisms of these alloys tribotesting against SiC ceramic balls under dry sliding process. Design/methodology/approach – Fe-Cr matrix alloys were fabricated using powder metallurgy route. The tribological behaviors of Fe-Cr alloys tribotesting against SiC ceramic balls using a ball-on-disc tribotester were studied at different testing conditions. Meanwhile, microstructure, phases and morphology of worn surfaces were investigated. Findings – The element boron improved mechanical properties and tribological behavior of alloys. The friction coefficients of Fe-Cr matrix alloys did not show obvious difference. The specific wear rates of alloys decreased and then increased because of the brittleness of alloys with the increase of boron content. Fe-21 weight per cent Cr-7 weight per cent B alloy showed the best tribological properties in dry sliding. The wear mechanism of Fe-Cr alloy ...

[1]  Wei-min Liu,et al.  Enhanced Ductility of Dendrite‐Ultrafine Eutectic Composite Fe3B Alloy Prepared by a Self‐Propagating High‐Temperature Synthesis , 2009 .

[2]  Y. Hibi,et al.  Friction and wear properties of Fe–Si intermetallic compounds in ethyl alcohol , 2012 .

[3]  J. L. Youngblood,et al.  Correlation of microstructure with mechanical properties of 300m steel , 1977 .

[4]  S. Yi,et al.  Sliding friction and wear behavior of Fe-based bulk metallic glass in 3.5% NaCl solution , 2010, Journal of Materials Science.

[5]  Wei-min Liu,et al.  Fabrication and study on tribological characteristics of bronze-alumina-silver composite under sea water condition , 2013 .

[6]  T. Furuhara,et al.  Relation between martensite morphology and volume change accompanying fcc to bcc martensitic transformation in Fe–Ni–Co alloys , 2006 .

[7]  A. H. Ucisik,et al.  Hard iron boride (Fe2B) on 99.97 wt% pure iron , 2006 .

[8]  A. Sorour,et al.  Microstructure and Tribology of Spark Plasma Sintered Fe–Cr–B Metamorphic Alloy Powder , 2011 .

[9]  C. G. Park,et al.  Microstructure and surface wear resistance in rapidly quenched Fe–Cr–B alloy spray coatings ☆ , 2001 .

[10]  K. Das,et al.  The abrasive wear resistance of TIC and (Ti,W)C-reinforced Fe–17Mn austenitic steel matrix composites , 2010 .

[11]  Weite Wu,et al.  Microstructural and abrasive characteristics of high carbon Fe–Cr–C hardfacing alloy , 2010 .

[12]  S. Kim,et al.  The effects of additive elements on the sliding wear behavior of Fe-base hardfacing alloys , 2003 .

[13]  L. Carpentier,et al.  Influence of intergranular metallic nanoparticles on the fretting wear mechanisms of Fe–Cr–Al2O3 nanocomposites rubbing on Ti–6Al–4V , 2008 .

[14]  M. Niu,et al.  Dry-Sliding Tribological Properties of Bronze–Graphite Composites , 2012, Tribology Letters.

[15]  H. Akbulut,et al.  Dry wear properties of A356-SiC particle reinforced MMCs produced by two melting routes , 2006 .

[16]  M. Maleque,et al.  The tribological behaviour of Fe-C-Al cast iron – effect of temperature , 2013 .

[17]  Wei-min Liu,et al.  Dry-sliding tribological properties of a nano-eutectic Fe1.87C0.13 alloy , 2010 .

[18]  Yimin Gao,et al.  Effect of 4wt.% Cr on microstructure, corrosion resistance and tribological properties of Fe3Al–20wt.%Al2O3 composites , 2013 .

[19]  P. S. Misra,et al.  Design and development of powder processed Fe–P based alloys , 2011 .

[20]  Shengyu Zhu,et al.  Tribological properties of bronze–graphite composites under sea water condition , 2012 .

[21]  Wei-min Liu,et al.  Dry-sliding Tribological Properties of Nano-Eutectic Fe83B17 Alloy , 2009 .

[22]  H. Fu,et al.  Effects of boron concentration on the corrosion resistance of Fe–B alloys immersed in 460 °C molten zinc bath , 2010 .

[23]  J. Archard Contact and Rubbing of Flat Surfaces , 1953 .

[24]  N. Yang,et al.  A new process for fabricating W-15 wt.%Cu sheet by sintering, cold rolling and re-sintering , 2010 .

[25]  Q. Xue,et al.  Tribocorrosion behavior of Ni-17.5Si-29.3Cr alloy in sulfuric acid solution , 2009 .