Novel High Temperature-Oxidation-Resistant Nanocomposites Developed by Nanocomposite Electrodeposition
暂无分享,去创建一个
[1] Y. Zhou,et al. Size Effect of Al Particles on the Oxidation of Electrodeposited Ni–Al Composite Coatings , 2005 .
[2] Cuimiao Zhang,et al. Hot Corrosion of an Electrodeposited Ni-11 wt % Cr Nanocomposite under Molten Na2SO4 – K2SO4 – NaCl , 2005 .
[3] Fu-hui Wang,et al. Oxidation of a novel electrodeposited Ni-Al nanocomposite film at 1050 °C , 2004 .
[4] Xinsheng Peng,et al. Development and oxidation at 800 °C of a novel electrodeposited Ni–Cr nanocomposite film , 2004 .
[5] X. Peng. Effect of La2O3 Particles on the Oxidation of Electrodeposited Nickel Films , 1999 .
[6] Xiaogang Peng,et al. Oxidation behavior of a Ni-LaO codeposited film on nickel , 1998 .
[7] R. Darolia,et al. NiAl alloys for high-temperature structural applications , 1991 .
[8] H. Lou,et al. Oxidation behaviour and scale morphology of normal-grained CoCrAl alloy and its sputtered microcrystalline coating , 1990 .
[9] John R. Nicholls,et al. High temperature corrosion , 1990 .
[10] J. Nicholls,et al. Optimising oxidation resistance of MCrAl coating systems using vapour phase alloy design , 1989 .
[11] G. Rybicki,et al. Effect of theθ-α-Al2O3 transformation on the oxidation behavior ofβ-NiAl + Zr , 1989 .
[12] G. Kitteringham. High Temperature Alloys for Gas Turbines and Other Applications 1986 , 1987 .
[13] M. Merz,et al. The oxidation resistance of fine-grained sputter-deposited 304 stainless steel , 1979 .