Transmission electron microscopic study of three-dimensional polyacrylonitrile fibre-mesophase pitch matrix carbon-carbon composite
暂无分享,去创建一个
[1] C. Ju,et al. Basal plane orientation of polyacrylonitrile fibers in a commercial polyacrylonitrile-pitch carbon-carbon composite , 1990 .
[2] J. Newman,et al. Petroleum-derived carbons , 1986 .
[3] H. Marsh,et al. Fracture mechanisms in microstrength testing of carbon artifacts , 1983 .
[4] J. Rouzaud,et al. Carbon films: Structure and microtexture (optical and electron microscopy, Raman spectroscopy) , 1983 .
[5] H. Marsh,et al. Structure in carbon/carbon fibre composites as studied by microscopy and etching with chromic acid , 1983 .
[6] A. Oberlin,et al. Characterization by electron microscopy of carbon phases (intermediate turbostratic phase and graphite) in hard carbons when heat-treated under pressure , 1980 .
[7] A. Oberlin,et al. Electron microscopic study on graphitization of bulk mesophases , 1978 .
[8] H. Marsh. Carbonization and liquid-crystal (mesophase) development: Part 1. The significance of the mesophase during carbonization of coking coals , 1973 .
[9] D. J. Johnson,et al. Observations of a three-phase structure in high-modulus PAN-based carbon fibres , 1973 .
[10] D. J. Johnson,et al. High‐resolution electron microscopy of high‐modulus carbon fibres * , 1971 .
[11] A. W. Baker,et al. Arbitrary techniques of band resolution—application to enthalpy calculations , 1966 .
[12] X. Bourrat,et al. Lattice imaging of disclinations in carbon fibers , 1990 .
[13] A. Oberlin,et al. Microtexture of nongraphitizing carbons and tem studies of some activated samples , 1990 .
[14] K. Sohn,et al. Failure behavior of carbon/carbon composites prepared by chemical vapor deposition , 1988 .
[15] Jai-Young Lee,et al. Effects of matrix structure on mechanical properties of carbon/carbon composites , 1988 .
[16] J. Jortner. Macroporosity and interface cracking in multi-directional carbon-carbons , 1986 .
[17] A. Oberlin,et al. Microtexture and structure of high temperature massive pyrocarbons prepared on graphite substrates , 1985 .
[18] H. Marsh,et al. Structure in graphitizable carbon from coal-tar pitch HTT 750–1148 K. Studied using high resolution electron microscopy , 1984 .
[19] J. White,et al. Mesophase alignment within carbon-fiber bundles , 1983 .
[20] D. Uhlmann,et al. Carbon mesophase-substrate interactions , 1983 .
[21] Y. Korai,et al. Catalytic graphitization of fibrous and particulate carbons , 1981 .
[22] J. Lahaye,et al. Characterization of carbon-carbon composites—I , 1981 .
[23] A. Oberlin,et al. Microtexture of mesophase spheres as studied by high resolution conventional transmission electron microscopy (CTEM) , 1980 .
[24] L. Manocha,et al. Influence of process parameters on the mechanical properties of carbon/carbon-composites with pitch as matrix precursor , 1980 .
[25] D. J. Johnson,et al. Electron-microscope studies of structural heterogeneity in pan-based carbon fibres , 1979 .
[26] Norman L. Allinger,et al. Conformational analysis—CI , 1974 .