Surface morphology evolution and ablation mechanism of SiC–Si multiphase ceramic coating on graphite under oxy-acetylene flame
暂无分享,去创建一个
[1] Hejun Li,et al. SiC coating toughened by HfC nanowires to protect C/C composites against oxidation , 2014 .
[2] Gao-hui Wu,et al. Microstructure and ablation mechanism of graphite/SiC composites under oxy-acetylene flame , 2014 .
[3] L. Chai,et al. Resistance to oxidation and ablation of SiC coating on graphite prepared by chemical vapor reaction , 2013 .
[4] Hejun Li,et al. ZrB2–SiC coating to protect carbon/carbon composites against ablation , 2013 .
[5] Qiang Zhang,et al. Ablation mechanisms of interpenetrating Al20Si/graphite composites , 2013 .
[6] Hejun Li,et al. Bamboo-shaped SiC nanowire-toughened SiC coating for oxidation protection of C/C composites , 2013 .
[7] Hejun Li,et al. Oxidation protection and behavior of C/C composites with an in situ SiC nanowire–SiC–Si/SiC–Si coating , 2013 .
[8] Wei Sun,et al. Ablation behavior of HfC protective coatings for carbon/carbon composites in an oxyacetylene combustion flame , 2012 .
[9] Hejun Li,et al. Toughening by SiC Nanowires in a Dense SiC–Si Ceramic Coating for Oxidation Protection of C/C Composites , 2012 .
[10] Ling-jun Guo,et al. Morphology, thermal response and anti-ablation performance of 3D-four directional pitch-based carbon/carbon composites , 2012 .
[11] Wei Sun,et al. Structural evolution and ablation mechanism of a hafnium carbide coating on a C/C composite in an oxyacetylene torch environment , 2012 .
[12] Hejun Li,et al. SiC/HfC/SiC ablation resistant coating for carbon/carbon composites , 2012 .
[13] Hejun Li,et al. Oxidation protection of C/C composites with a multilayer coating of SiC and Si + SiC + SiC nanowires , 2012 .
[14] Hejun Li,et al. Oxidation protection of SiC-coated C/C composites by SiC nanowire-toughened CrSi2–SiC–Si coating , 2012 .
[15] Li Kezhi,et al. Effect of SiC Nanowires on the Mechanical and Oxidation Protective Ability of SiC Coating for C/C Composites , 2012 .
[16] Hejun Li,et al. SiC coating toughened by SiC nanowires to protect C/C composites against oxidation , 2012 .
[17] Hejun Li,et al. Preparation and ablation properties of ZrC-SiC coating for carbon/carbon composites by solid phase infiltration , 2011 .
[18] Hejun Li,et al. Influence of SiC nanowires on the properties of SiC coating for C/C composites between room temperature and 1500 °C , 2011 .
[19] G. Wen,et al. Formation of ZrC ablation protective coatings on carbon material by tungsten inert gas cladding technique , 2010 .
[20] Wei Sun,et al. ZrC ablation protective coating for carbon/carbon composites , 2009 .
[21] Heng Wu,et al. A Si―SiC oxidation protective coating for carbon/carbon composites prepared by a two-step pack cementation , 2009 .
[22] W. Bo,et al. SiCn/SiC oxidation protective coating for carbon/carbon composites , 2009 .
[23] Hejun Li,et al. A MoSi2–SiC–Si oxidation protective coating for carbon/carbon composites , 2007 .
[24] Leonard C. Feldman,et al. Modified Deal Grove model for the thermal oxidation of silicon carbide , 2004 .
[25] Huang Jianfeng,et al. Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C composites , 2004 .
[26] H. Fukuda,et al. SiC/C multi-layered coating contributing to the antioxidation of C/C composites and the suppression of through-thickness cracks in the layer , 2001 .
[27] Donghwan Cho,et al. Microstructural interpretation of the effect of various matrices on the ablation properties of carbon-fiber-reinforced composites , 2001 .
[28] N. Iwamoto,et al. Formation of a functionally gradient (Si3N4+SiC)/C layer for the oxidation protection of carbon-carbon composites , 1999 .
[29] Shanyi Du,et al. Oxidation and ablation of 3D carbon-carbon composite at up to 3000 °C , 1995 .
[30] G. Springer,et al. High Temperature Thermomechanical Behavior of Carbon-Phenolic and Carbon-Carbon Composites, I. Analysis , 1992 .
[31] D. Schmidt. Ablative Polymers in Aerospace Technology , 1969 .
[32] A. S. Grove,et al. General Relationship for the Thermal Oxidation of Silicon , 1965 .