Characterization of latticed SiC nanowires containing coating for carbon foam using carbonization activated pack cementation process

[1]  H. Mei,et al.  Mechanical, structural and oxidation resistance enhancement of carbon foam by in situ grown SiC nanowires , 2016 .

[2]  S. Farhan,et al.  A novel method for the processing of carbon foam containing in situ grown nano-materials and silicon nanowires , 2015 .

[3]  Wei Sun,et al.  Ablation behavior of ZrB2–SiC protective coating for carbon/carbon composites , 2015 .

[4]  S. Farhan,et al.  Thermal, mechanical and self-destruction properties of aluminum reinforced carbon foam , 2015, Journal of Porous Materials.

[5]  Hejun Li,et al.  Ablation resistance of ZrB2–SiC coating prepared by supersonic atmosphere plasma spraying for SiC-coated carbon/carbon composites , 2014 .

[6]  Noaman Ul‐Haq,et al.  Preparation and characterization of carbon foam derived from pitch and phenolic resin using a soft templating method , 2014 .

[7]  Hejun Li,et al.  SiC coating toughened by HfC nanowires to protect C/C composites against oxidation , 2014 .

[8]  Bin Zhang,et al.  Synthesis of β-SiC nanowires by ball milled nanoparticles of silicon and carbon , 2014 .

[9]  Hejun Li,et al.  ZrB2–SiC gradient oxidation protective coating for carbon/carbon composites , 2014 .

[10]  K. Svoboda,et al.  Ammonia yield from gasification of biomass and coal in fluidized bed reactor , 2014 .

[11]  Jianfeng Huang,et al.  A mullite/SiC oxidation protective coating for carbon/carbon composites , 2013 .

[12]  Hejun Li,et al.  Toughening by SiC Nanowires in a Dense SiC–Si Ceramic Coating for Oxidation Protection of C/C Composites , 2012 .

[13]  Hejun Li,et al.  A SiC–Si–ZrB2 multiphase oxidation protective ceramic coating for SiC-coated carbon/carbon composites , 2012 .

[14]  Chengguo Wang,et al.  Fabrication of a SiC/Si/MoSi2 multi-coating on graphite materials by a two-step technique , 2012 .

[15]  Li Kezhi,et al.  Effect of SiC Nanowires on the Mechanical and Oxidation Protective Ability of SiC Coating for C/C Composites , 2012 .

[16]  Hejun Li,et al.  SiC coating toughened by SiC nanowires to protect C/C composites against oxidation , 2012 .

[17]  H. Sano,et al.  A carbon nanotube–enhanced SiC coating for the oxidation protection of C/C composite materials , 2011 .

[18]  B. Drevet,et al.  Resistance to oxidation of graphite silicided by reactive infiltration , 2011 .

[19]  Hejun Li,et al.  Influence of SiC nanowires on the properties of SiC coating for C/C composites between room temperature and 1500 °C , 2011 .

[20]  Hejun Li,et al.  A modified dual-layer SiC oxidation protective coating for carbon/carbon composites prepared by one-step pack cementation , 2011 .

[21]  Q. Guo,et al.  Preparation of phenolic-based carbon foam with controllable pore structure and high compressive strength , 2010 .

[22]  X. Hou,et al.  A simple model for the oxidation of carbon-containing composites , 2010 .

[23]  Sung-Churl Choi,et al.  In situ growth of SiC nanowires by carbothermal reduction using a mixture of low-purity SiO2 and carbon , 2008 .

[24]  D. Frenkel,et al.  State-of-the-art models for the phase diagram of carbon and diamond nucleation , 2008, 0804.1671.

[25]  Lang Liu,et al.  Microstructure and property of SiC coating for carbon materials , 2007 .

[26]  Hejun Li,et al.  A C/SiC gradient oxidation protective coating for carbon/carbon composites , 2006 .

[27]  Alfred H. Stiller,et al.  Carbon foam derived from various precursors , 2006 .

[28]  Hejun Li,et al.  Yttrium silicate oxidation protective coating for SiC coated carbon/carbon composites , 2006 .

[29]  Yong Yang,et al.  Iron-catalytic growth of prism-shaped single-crystal silicon nanowires by chemical vapor deposition of silane , 2005 .

[30]  Xiaohong Shi,et al.  Silicon carbide coating to protect carbon/carbon composites against oxidation , 2005 .

[31]  Huang Jianfeng,et al.  Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C composites , 2004 .

[32]  Noriaki Sano,et al.  Separated synthesis of iron-included carbon nanocapsules and nanotubes by pyrolysis of ferrocene in pure hydrogen , 2003 .

[33]  David P. Anderson,et al.  Graphitic open-celled carbon foams: processing and characterization , 2003 .

[34]  Huang Jianfeng,et al.  Mullite-Al2O3-SiC oxidation protective coating for carbon/carbon composites , 2003 .

[35]  D.D.L. Chung,et al.  Oxidation protection of carbon materials by acid phosphate impregnation , 2002 .

[36]  P. Molian,et al.  A novel laser technique for oxidation-resistant coating of carbon-carbon composite , 2001 .

[37]  Yasuhiro Ohshima,et al.  Enhancement of N2 formation from the nitrogen in carbon and coal by calcium , 2001 .

[38]  R. Banerjee,et al.  Effect of the size-induced structural transformation on the band gap in CdS nanoparticles , 2000 .

[39]  Zhiheng Wu,et al.  Effect of Calcium Catalyst on Coal Nitrogen Removal during Pyrolysis , 2000 .

[40]  S. Fan,et al.  Growth of SiC nanorods prepared by carbon nanotubes-confined reaction , 2000 .

[41]  V. Zaikovskii,et al.  Study of multiwalled graphite nanotubes and filaments formation from carbonized products of polyvinyl alcohol via catalytic graphitization at 600–800°C in nitrogen atmosphere , 2000 .

[42]  J. Cawley,et al.  Effect of Stacking Faults on the X-Ray Diffraction Profiles of Beta-SiC Powders , 1995 .

[43]  K. A. Trick,et al.  Mechanisms of the pyrolysis of phenolic resin in a carbon/phenolic composite , 1995 .

[44]  J. Sheehan,et al.  Carbon-Carbon Composites , 1994 .

[45]  L. Allard,et al.  Synthesis and characterization of SiC whiskers , 1992 .