Steam oxidation of TP347HFG, super 304H and HR3C – analysis of significance of steam flowrate and specimen surface finish

Abstract This paper delivers an analysis of the steam oxidation of the austenitic steels used for the super heater and re-heater tubing. It compares the behaviour of TP347HFG, Super 304H and HR3C at 650 and 700°C with three different steam flowrates: 4, 16· 40 mm/s. Steam oxidation tests were performed in closed loop system for 1000 h. The differences in the steam oxidation behaviour of these materials are considered in terms of the alloy compositions (especially chromium content), the steam flowrate and the material surface finish.

[1]  Jan-Erik Svensson,et al.  Influence of Water Vapor and Flow Rate on the High-Temperature Oxidation of 304L; Effect of Chromium Oxide Hydroxide Evaporation , 2000 .

[2]  I. Wright,et al.  An Assessment of the High Temperature Oxidation Behavior of Fe-Cr Steels in Water Vapor and Steam , 2002 .

[3]  Jan-Erik Svensson,et al.  Evidence for Chromium Evaporation Influencing the Oxidation of 304L: The Effect of Temperature and Flow Rate , 2002 .

[4]  L. Singheiser,et al.  Oxidation limited life times of chromia forming ferritic steels , 2004 .

[5]  S. A. Jensen,et al.  Investigation on steam oxidation behaviour of TP347H FG Part 1: Exposure at 256 bar , 2005 .

[6]  L. Singheiser,et al.  Effect of component thickness on lifetime and oxidation rate of chromia forming ferritic steels in low and high pO2 environments , 2005 .

[7]  J. Svensson,et al.  Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600 °C , 2006 .

[8]  R. Viswanathan,et al.  Boiler materials for ultra-supercritical coal power plants—Steamside oxidation , 2006 .

[9]  M. Montgomery,et al.  Steam Oxidation of TP 347H FG in Power Plants , 2006 .

[10]  D. Young Effects of Water Vapour on the Oxidation of Chromia Formers , 2008 .

[11]  G. Dong,et al.  BCNO-Based Long-Persistent Phosphor , 2009 .

[12]  L. Singheiser,et al.  Effect of specimen thickness on the growth rate of chromia scales on Ni-base alloys in high- and low-pO2 gases , 2009 .

[13]  Gordon R. Holcomb,et al.  Steam Oxidation and Chromia Evaporation in Ultrasupercritical Steam Boilers and Turbines , 2009 .

[14]  M. Montgomery,et al.  Development of the inner oxide zone upon steam oxidation of an austenitic stainless steel , 2009 .

[15]  I. Wright,et al.  A review of the oxidation behaviour of structural alloys in steam , 2010 .

[16]  F. Grumsen,et al.  Microstructure Evolution During Steam Oxidation of a Nb Stabilized Austenitic Stainless Steel , 2010 .

[17]  J. Nicholls,et al.  Characterisation of oxide scales developed on high temperature resistant alloys in pure steam environments , 2012 .