Antibacterial activity of kaolinite/nanoTiO2 composites in relation to irradiation time.

The paper addresses laboratory preparation and antibacterial activity testing of kaolinite/nanoTiO2 composite in respect of the daylight irradiation time. Kaolinite/nanoTiO2 composites with 20 and 40 wt% of TiO2 were laboratory prepared, dried at 105 °C and calcined at 600 °C. The calcination caused transformation of kaolinite to metakaolinite and origination of the metakaolinite/nanoTiO2 composite. X-ray powder diffraction, Raman and FTIR spectroscopic methods revealed titanium dioxide only in the form of anatase in all evaluated samples (non-calcined and calcined) and also transformation of kaolinite to metakaolinite after the calcination treatment. Scanning electron microscopy was used as a method for characterization of morphology and elemental composition of the studied samples. A standard microdilution test was used to determine the antibacterial activity using four human pathogenic bacterial strains (Staphylococcus aureus, Escherichia coli, Enterococcus faecalis, Pseudomonas aeruginosa). A lamp with a wide spectrum bulb simulating daylight was used for induction of photocatalysis. The antibacterial assays found all the KATI samples to have antibacterial potency with different onset of the activity when calcined samples exhibited antibacterial activity earlier than the non-calcined. Significant difference in antibacterial activity of KATI samples for different bacterial strains was not observed.

[1]  C. Saint,et al.  Synthesis and characterisation of novel titania impregnated kaolinite nano-photocatalyst , 2009 .

[2]  V. Matějka,et al.  Preparation and characterization of photoactive composite kaolinite/TiO(2). , 2011, Journal of hazardous materials.

[3]  Cesar Pulgarin,et al.  Photocatalytical inactivation of E. coli: effect of (continuous-intermittent) light intensity and of (suspended-fixed) TiO2 concentration , 2003 .

[4]  Mark J. Hampden-Smith,et al.  The formation of titanium oxide monolayer coatings on silica surfaces , 1991 .

[5]  Chi Sun Poon,et al.  Photocatalytic construction and building materials: From fundamentals to applications , 2009 .

[6]  Karel Frydrýšek,et al.  Design of External Fixators used in Traumatology and Orthopaedics – Treatment of Fractures of Pelvis and its Acetabulum , 2012 .

[7]  Akira Fujishima,et al.  Titanium dioxide photocatalysis , 2000 .

[8]  G. Kakali,et al.  Thermal treatment of kaolin : the effect of mineralogy on the pozzolanic activity , 2001 .

[9]  Konstantin Kovler,et al.  The effect of dehydroxylation/amorphization degree on pozzolanic activity of kaolinite , 2003 .

[10]  W. Jacoby,et al.  Microfibrous Mesh Coated with Titanium Dioxide: A Self-Sterilizing, Self-Cleaning Filter , 2002, Journal of the Air & Waste Management Association.

[11]  R. Bauer,et al.  Photocatalytic oxidation of gaseous chlorinated organics over titanium dioxide. , 2000, Chemosphere.

[12]  I. Dékány,et al.  Structural and photooxidation properties of SnO2/layer silicate nanocomposites , 2004 .

[13]  A. Nakajima,et al.  Preparation and properties of TiO2/montmorillonite composites , 2009 .

[14]  H. W. Van der Marel,et al.  Atlas of Infrared Spectroscopy of Clay Minerals and Their Admixtures , 1976 .

[15]  W. Fischer H.W. van der Marel und H. Beutelspacher (Herausg.): Atlas of infrared spectroscopy of clay minerals and their admixtures. Elsevier, Amsterdam 1976. VIII + 396 Seiten, Großformat Dfl. 165,— , 1977 .

[16]  I. Dékány,et al.  Zinc oxide nanoparticles incorporated in ultrathin layer silicate films and their photocatalytic properties , 2003 .

[17]  Chia-Yu Lin,et al.  Inactivation of Microorganisms on the Photocatalytic Surfaces in Air , 2003 .

[18]  L. N. Arakaki,et al.  Removal of cadmium, zinc, manganese and chromium cations from aqueous solution by a clay mineral. , 2006, Journal of hazardous materials.

[19]  Karen Scrivener,et al.  The origin of the pozzolanic activity of calcined clay minerals: A comparison between kaolinite, illite and montmorillonite , 2011 .

[20]  R. Lago,et al.  Floating photocatalysts based on TiO2 supported on high surface area exfoliated vermiculite for water decontamination , 2006 .

[21]  L. Rintoul,et al.  Lattice vibrations of montmorillonite: an FT Raman and X-ray diffraction study , 1996 .

[22]  Q. Huang,et al.  The effect of extracellular polymeric substances on the adhesion of bacteria to clay minerals and goethite , 2013 .

[23]  A. Matthews,et al.  Growth behavior and microstructure of arc ion plated titanium dioxide , 2009 .

[24]  Tiina Reponen,et al.  Control of aerosol contaminants in indoor air: combining the particle concentration reduction with microbial inactivation. , 2007, Environmental science & technology.

[25]  K. Jan,et al.  Ultrafine titanium dioxide particles in the absence of photoactivation can induce oxidative damage to human bronchial epithelial cells. , 2005, Toxicology.

[26]  V. Matějka,et al.  Vermiculite interlayer as a reactor for CdS ultrafine particles preparation , 2010 .