Abstract Geometrical conditions of spacer grid springs and dimples of a light water reactor fuel assembly are studied in this paper concerning a fuel rod’s fretting wear failure. In this framework, the springs/dimples are categorized from the aspects of their orientation with respect to the fuel axis and the contact types. Possible motions on the contacts between the springs/dimples and fuel rods are estimated by conducting a flow-induced vibration test. Features of the wear scar and depth are investigated by independent fretting wear tests carried out with spring and dimple specimens of typical contact geometries. It is also attempted here to apply the contact mechanics theory to a fuel fretting wear analysis such as the prediction of a wear depth profile and its rate, which is influenced by the contact shape of the springs/dimples. It is shown that the theory can be applied to a dimensional control of a coining for the springs/dimples, which is usually carried out in a thin plate fabrication. From the results, the necessary conditions for a spring/dimple geometry for restraining a fretting wear failure are discussed.
[1]
M. J. Pettigrew,et al.
Flow-induced vibration : recent findings and open questions
,
1998
.
[2]
J. Archard.
Contact and Rubbing of Flat Surfaces
,
1953
.
[3]
David A. Hills,et al.
Mechanics of elastic contacts
,
1993
.
[4]
M. Godet.
The third-body approach: A mechanical view of wear
,
1984
.
[5]
Michele Ciavarella,et al.
On non-symmetrical plane contacts
,
1999
.
[6]
Hyung-Kyu Kim,et al.
Fretting wear of laterally supported tube
,
2001
.