Improving surface finish and wear resistance of additive manufactured nickel-titanium by ultrasonic nano-crystal surface modification
暂无分享,去创建一个
Gary L. Doll | Ahmadreza Jahadakbar | Mohammad Elahinia | Chang Ye | Narges Shayesteh Moghaddam | M. Elahinia | N. Moghaddam | M. T. Andani | Hao Zhang | Z. Ren | Yalin Dong | Chang Ye | Ahmadreza Jahadakbar | G. Doll | Hamdy Ibrahim | Haifeng Qin | Mohsen Taheri Andani | Chi Ma | Chi Ma | Hamdy Ibrahim | Haifeng Qin | Zhencheng Ren | Hao Zhang | Amirehesam Amerinatanzi | Yalin Dong | A. Amerinatanzi | N. S. Moghaddam
[1] Fang-Jung Shiou,et al. Freeform surface finish of plastic injection mold by using ball-burnishing process , 2003 .
[2] Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties , 2012 .
[3] S. Stupp,et al. Porous NiTi for bone implants: a review. , 2008, Acta biomaterialia.
[4] D. Qian,et al. Surface grain boundary engineering of Alloy 600 for improved resistance to stress corrosion cracking , 2015 .
[5] Robert L. Mason,et al. Fatigue Life of Titanium Alloys Fabricated by Additive Layer Manufacturing Techniques for Dental Implants , 2013, Metallurgical and Materials Transactions A.
[6] Moataz M. Attallah,et al. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V , 2013 .
[7] M. Elahinia,et al. The influence of heat treatment on the thermomechanical response of Ni-rich NiTi alloys manufactured by selective laser melting , 2016 .
[8] M. Zhu,et al. Corrosion behaviour of nanocrystalline 304 stainless steel prepared by equal channel angular pressing , 2012 .
[9] Amirhesam Amerinatanzi,et al. Fabrication of NiTi through additive manufacturing: A review , 2016 .
[10] Hashem Ashrafiuon,et al. Nonlinear Control of a Shape Memory Alloy Actuated Manipulator , 2002 .
[11] P. Colegrove,et al. Microstructure and Mechanical Properties of Wire and Arc Additive Manufactured Ti-6Al-4V , 2013, Metallurgical and Materials Transactions A.
[12] M. Elahinia,et al. Manufacturing and processing of NiTi implants: A review , 2012 .
[13] J. Kruth,et al. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V , 2010 .
[14] R. Balasubramaniam,et al. Properties of passive film formed on CP titanium, Ti–6Al–4V and Ti–13.4Al–29Nb alloys in simulated human body conditions , 2005 .
[15] Mohammad Elahinia,et al. Shape Memory Alloy Actuators: Design, Fabrication, and Experimental Evaluation , 2015 .
[16] Mohammad Elahinia,et al. Design, modeling and experimental evaluation of a minimally invasive cage for spinal fusion surgery utilizing superelastic Nitinol hinges , 2015 .
[17] Mary C. Boyce,et al. Effects of strain rate, temperature and thermomechanical coupling on the finite strain deformation of glassy polymers , 1995 .
[18] David Dean,et al. Metals for bone implants. Part 1. Powder metallurgy and implant rendering. , 2014, Acta biomaterialia.
[19] M. Elahinia,et al. Additive Manufacturing of Nitinol Shape Memory Alloys to Overcome Challenges in Conventional Nitinol Fabrication , 2014 .
[20] M. Es‐Souni,et al. On the properties of two binary NiTi shape memory alloys. Effects of surface finish on the corrosion behaviour and in vitro biocompatibility. , 2002, Biomaterials.
[21] L. Yahia,et al. Effect of modification of oxide layer on NiTi stent corrosion resistance. , 1998, Journal of biomedical materials research.
[22] M. Ramulu,et al. Fatigue performance evaluation of selective laser melted Ti–6Al–4V , 2014 .
[23] Juan de Lara,et al. Supporting user-oriented analysis for multi-view domain-specific visual languages , 2009, Inf. Softw. Technol..
[24] Zhong Zhou,et al. Gradient nanostructure and residual stresses induced by Ultrasonic Nano-crystal Surface Modification in 304 austenitic stainless steel for high strength and high ductility , 2014 .
[25] Y. Pyun,et al. Fretting wear and friction reduction of CP titanium and Ti–6Al–4V alloy by ultrasonic nanocrystalline surface modification , 2012 .
[26] Mohammad Elahinia,et al. Texture, aging, and superelasticity of selective laser melting fabricated Ni-rich NiTi alloys , 2017 .
[27] D. Qian,et al. Surface amorphization of NiTi alloy induced by Ultrasonic Nanocrystal Surface Modification for improved mechanical properties. , 2016, Journal of the mechanical behavior of biomedical materials.
[28] Ri-ichi Murakami,et al. Fatigue properties of a S45C steel subjected to ultrasonic nanocrystal surface modification , 2010 .
[29] Florencia Edith Wiria,et al. Property enhancement of 3D-printed alumina ceramics using vacuum infiltration , 2014 .
[30] M. Atai,et al. The Influence of Surface Nanocrystallization Induced by Shot Peening on Corrosion Behavior of NiTi Alloy , 2015, Journal of Materials Engineering and Performance.
[31] K. Hayashi,et al. Evaluation of carcinogenicity and chronic toxicity associated with orthopedic implants in mice. , 1994, Journal of biomedical materials research.
[32] Ri-ichi Murakami,et al. Improvement of the fatigue strength of SUS304 austenite stainless steel using ultrasonic nanocrystal surface modification , 2013 .
[33] Horst Meier,et al. On the development of high quality NiTi shape memory and pseudoelastic parts by additive manufacturing , 2014 .
[34] E. Denkhaus,et al. Nickel essentiality, toxicity, and carcinogenicity. , 2002, Critical reviews in oncology/hematology.