Study on water sorptivity of the surface layer of concrete

[1]  Zongjin Li,et al.  Multi-Aggregate Approach for Modeling Interfacial Transition Zone in Concrete , 2014 .

[2]  Zongjin Li,et al.  Realistic pore structure of Portland cement paste: experimental study and numerical simulation , 2013 .

[3]  A. Rajor,et al.  Influence of bacteria on the compressive strength, water absorption and rapid chloride permeability of concrete incorporating silica fume , 2012 .

[4]  R. Talero,et al.  Morphological Differentiation and Crystal Growth Form of Friedel's Salt Originated from Pozzolan and Portland Cement , 2012 .

[5]  Jean Talandier,et al.  Water retention and gas relative permeability of two industrial concretes , 2012 .

[6]  W. Müllauer,et al.  Effect of carbonation, chloride and external sulphates on the leaching behaviour of major and trace elements from concrete , 2012 .

[7]  J. Weiss,et al.  Water Absorption and Critical Degree of Saturation Relating to Freeze-Thaw Damage in Concrete Pavement Joints , 2012 .

[8]  D. Panesar,et al.  The effect of short duration NaCl exposure on the surface pore structure of concrete containing GGBFS , 2012 .

[9]  Seung-Jun Kwon,et al.  Modeling of water permeability in early aged concrete with cracks based on micro pore structure , 2012 .

[10]  Masanobu Shinozuka,et al.  Prediction of corrosion initiation in reinforced concrete members subjected to environmental stressors: A finite‐element framework , 2012 .

[11]  Stéphane Poyet,et al.  Assessment of the unsaturated water transport properties of an old concrete: Determination of the pore-interaction factor , 2011 .

[12]  D. Bentz,et al.  Effect of sample conditioning on the water absorption of concrete , 2011 .

[13]  Toyoharu Nawa,et al.  Effect of fly ash on the kinetics of Portland cement hydration at different curing temperatures , 2011 .

[14]  D. Cleland,et al.  Durability and water absorption properties of surface treated concretes , 2011 .

[15]  C. Qian,et al.  Experiment study of chemo-mechanical coupling behavior of leached concrete , 2011 .

[16]  Mohammad Pour-Ghaz,et al.  Wetting and drying of concrete using aqueous solutions containing deicing salts , 2011 .

[17]  T. Scherer,et al.  Protective or damage promoting effect of calcium carbonate layers on the surface of cement based materials in aqueous environments , 2010 .

[18]  Barbara Lothenbach,et al.  Impact of chloride on the mineralogy of hydrated portland cement systems , 2010 .

[19]  Alaa M. Rashad,et al.  Durability and strength evaluation of high-performance concrete in marine structures , 2010 .

[20]  Fabrice Deby,et al.  Probabilistic approach for durability design of reinforced concrete in marine environment , 2009 .

[21]  P. Basheer,et al.  The influence of reusing ‘Formtex’ controlled permeability formwork on strength and durability of concrete , 2008 .

[22]  Mario Plos,et al.  Bond behaviour of corroded reinforcing steel bars in concrete , 2006 .

[23]  K. Aligizaki Pore Structure of Cement-Based Materials: Testing, Interpretation and Requirements , 2005 .

[24]  S. Nagasaki,et al.  Change In Pore Structure And Composition Of Hardened Cement Paste During The Process Of Dissolution , 2005 .

[25]  P. Brown,et al.  The system CaO-Al2O3-CaCl2-H2O at 23±2 °C and the mechanisms of chloride binding in concrete , 2004 .

[26]  Jeffrey J. Thomas,et al.  Effects of Decalcification on the Microstructure and Surface Area of Cement and Tricalcium Silicate Pastes | NIST , 2004 .

[27]  Min-Hong Zhang,et al.  Water permeability and chloride penetrability of high-strength lightweight aggregate concrete , 2002 .

[28]  Sidney Diamond,et al.  Mercury porosimetry: An inappropriate method for the measurement of pore size distributions in cement-based materials , 2000 .

[29]  R. Hooton,et al.  Effects of fresh water exposure on chloride contaminated concrete , 2000 .

[30]  C. Poon,et al.  Degree of hydration and gel/space ratio of high-volume fly ash/cement systems , 2000 .

[31]  F. P. Glasser,et al.  Friedel’s salt, Ca2Al(OH)6(Cl,OH)·2H2O: its solid solutions and their role in chloride binding , 1998 .

[32]  Raoul François,et al.  Effect of the leaching of calcium hydroxide from cement paste on mechanical and physical properties , 1997 .

[33]  F. Adenot,et al.  Leaching of cement: Study of the surface layer , 1996 .

[34]  F. R. Montgomery,et al.  The Autoclam - a new test for permeability , 1994 .

[35]  J. Bijen,et al.  The reaction of fly ash in concrete a critical examination , 1989 .

[36]  Hongyan Ma Multi-scale modeling of the microstructure and transport properties of contemporary concrete , 2013 .

[37]  H. Ludwig,et al.  Field performance of concrete exposed to sulphate and low pH conditions from natural and industrial sources , 2012 .

[38]  Y. Cai,et al.  Study of chloride binding and diffusion in GGBS concrete , 2003 .

[39]  S. Pii FRIEDEL'S SALT, Ca2Al(OH)6(Cl,OH)z2H2O: ITS SOLID SOLUTIONS AND THEIR ROLE IN CHLORIDE BINDING , 1998 .

[40]  A. Neville,et al.  PROPERTIES OF CONCRETE. 4TH AND FINAL EDITION , 1995 .

[41]  A C Smith,et al.  Corrosion of steel in concrete , 1982 .

[42]  E. Barrett,et al.  (CONTRIBUTION FROM THE MULTIPLE FELLOWSHIP OF BAUGH AND SONS COMPANY, MELLOX INSTITUTE) The Determination of Pore Volume and Area Distributions in Porous Substances. I. Computations from Nitrogen Isotherms , 1951 .