Effect of Oxygen Partial Pressure on Silver Migration of Low-Temperature Sintered Nanosilver Die-Attach Material

The low-temperature joining technique of silver sintering is being actively pursued in the power electronics industry as a lead-free die-attach solution for packaging power devices and modules. However, one of the concerns of this technique is the migration of silver at a high temperature. Recently, we have reported our findings of the migration of a low-temperature sintered nanosilver in dry air at a temperature over 250°1C. In this paper, we report our results of the effect of oxygen partial pressure on the migration kinetics of the sintered nanosilver at 400°C under an electrical field strength of 50 V/mm. The range of the oxygen partial pressure tested was between <; 0.01 and 0.40 atm. The silver migration kinetics were monitored by measuring the leakage current across a metal-finger pattern, which allowed the determination of the "lifetime," or the onset time for significant leakage current developed across the two electrodes. With decreasing oxygen partial pressure, the lifetime increases exponentially. Our results suggest that the concern for silver migration in a high-temperature application of sintered silver die attach can be effectively remedied through packaging to keep oxygen away from the silver joints.

[1]  D. A. Love,et al.  Rapid migration of silver on roughened glass surfaces in a methanol/air mixture near 500 °C , 1995 .

[2]  H. Naguib,et al.  Silver Migration and the Reliability of Pd/Ag Conductors in Thick-Film Dielectric Crossover Structures , 1979 .

[3]  G. T. Kohman,et al.  Silver migration in electrical insulation , 1955 .

[4]  Uwe Scheuermann,et al.  The Road to the Next Generation Power Module - 100% Solder Free Design , 2008 .

[5]  Silver Migration in Glass Dams between Silver-Palladium Interconnections , 1975, IEEE Transactions on Electrical Insulation.

[6]  G. Lu,et al.  Sintered nanosilver paste for high-temperature power semiconductor device attachment , 2009 .

[7]  Sears,et al.  Measurements of the electrical mobility of silver over a hot tin oxide surface. , 1993, Physical review. B, Condensed matter.

[8]  Tao Wang,et al.  Low-Temperature Sintering with Nano-Silver Paste in Die-Attached Interconnection , 2007 .

[9]  Guo-Quan Lu,et al.  Thermomechanical Reliability of Low-Temperature Sintered Silver Die Attached SiC Power Device Assembly , 2006, IEEE Transactions on Device and Materials Reliability.

[10]  R. Sittig,et al.  Top-side chip contacts with low temperature joining technique (LTJT) , 2004, 2004 IEEE 35th Annual Power Electronics Specialists Conference (IEEE Cat. No.04CH37551).

[11]  Xu Chen,et al.  Low-temperature and Pressureless Sintering Technology for High-performance and High-temperature Interconnection of Semiconductor Devices , 2007, 2007 International Conference on Thermal, Mechanical and Multi-Physics Simulation Experiments in Microelectronics and Micro-Systems. EuroSime 2007.

[12]  Rolf E. Hummel,et al.  ON THE DIRECTION OF ELECTROMIGRATION IN THIN SILVER, GOLD, AND COPPER FILMS , 1971 .

[13]  Jing-Chie Lin,et al.  On the resistance of silver migration in Ag-Pd conductive thick films under humid environment and applied d.c. field , 1996 .

[14]  G. Lu,et al.  Low-Temperature Sintering of Nanoscale Silver Paste for Power Chip Attachment , 2008 .

[15]  Guo-Quan Lu,et al.  Low-Temperature Sintered Nanoscale Silver as a Novel Semiconductor Device-Metallized Substrate Interconnect Material , 2006, IEEE Transactions on Components and Packaging Technologies.

[16]  J. Gagne Silver Migration Model for Ag-Au-Pd Conductors , 1982 .