Comparison of Development Length Equation of Bottom and Top GFRP Bars with Splitting Failure
暂无分享,去创建一个
The objective of this study was to propose a development length equation for bottom and top GFRP bars. Including the bottom and top GRPP bars, a total of 104 modified pullout tests were completed. The test variables were embedment length (15, 30, 45db), net cover thickness (0.5~2.0db), different GFRP bar types, and bar diameters (10, 13, 16mm). The average bond stresses were determined based on the modified pullout test results. Two variable linear regression analyses were performed on the results of the average bond stresses. Utilizing the 5% fractile concept, a conservative development length design equation was derived. The design equation of the development length for bottom and top GFRP bars was proposed and the design equation derived in this study was compared to the ACI 440.1R-06 committee equation.
[1] H. Saadatmanesh,et al. Design Recommendations for Bond of GFRP Rebars to Concrete , 1996 .
[2] Carol K. Shield,et al. Development Length of Glass Fiber-Reinforced Polymer Bars in Concrete , 2006 .
[3] S. Ha,et al. Splice Length of GFRP Rebars Based on Flexural Tests of Unconfined RC Members , 2009 .
[4] Jong-Pil Won,et al. Recommendations of Environmental Reduction Factor of FRP Rebar for Durability Design of Concrete Structure , 2004 .