Fabrication and oxidation behavior of Cr(2)AlC coating on Ti6242 alloy

An similar to 5 mu m Cr(2)AlC coating was synthesized on near-a titanium alloy Ti6242 using an industrially sized magnetron sputtering coater. Isothermal oxidation at 700 degrees C and 800 degrees C, and cyclic oxidation at 700 degrees C of the bare alloys and coated specimens were investigated in air. The results indicated that the Ti6242 alloy faced serious oxidation problems at 700 degrees C and 800 degrees C. Repeated formation and spallation of the multilayered oxide scale on the Ti6242 alloy occurred during oxidation testing. The coated specimens exhibited much better oxidation behaviour as compared to the bare alloy. A continuous Al-rich oxide scale formed on the coating surface during the initial oxidation stages. The oxide scale and coating itself acted as diffusion barriers blocking the further ingress of oxygen and protected the substrate alloy from oxidation. The oxidation mechanisms of the bare alloy and the coated specimens were investigated based on the experimental results. (C) 2010 Elsevier BM. All rights reserved.

[1]  T. Nguyen,et al.  Cyclic oxidation of Cr2AlC between 1000 and 1300 °C in air , 2008 .

[2]  Michel W. Barsoum,et al.  The MN+1AXN phases: A new class of solids , 2000 .

[3]  M. Barsoum,et al.  Long Time Oxidation Study of Ti3SiC2 , Ti3SiC2 / SiC , and Ti3SiC2 / TiC Composites in Air , 2003 .

[4]  Ola Wilhelmsson,et al.  Growth and characterization of MAX-phase thin films , 2005 .

[5]  C. Leyens,et al.  Influence of microstructure on oxidation behaviour of near-α titanium alloys , 1996 .

[6]  C. Leyens,et al.  Oxidation and Protection of Near-Alpha Titanium Alloys , 1997 .

[7]  Zushu Hu,et al.  Effect of the θ–α-Al2O3 Transformation in Scales on the Oxidation Behavior of a Nickel-Base Superalloy with an Aluminide Diffusion Coating , 2000 .

[8]  M. Radovic,et al.  Microstructure and Residual Stress of Alumina Scale Formed on Ti2AlC at High Temperature in Air , 2007 .

[9]  R. Ahuja,et al.  Deposition and characterization of ternary thin films within the Ti–Al–C system by DC magnetron sputtering , 2006 .

[10]  M. Barsoum,et al.  Oxidation of Ti3SiC2 in air , 1997 .

[11]  S. Lofland,et al.  Synthesis and characterization of Nb2AlC thin films , 2009 .

[12]  U. Jansson,et al.  Structural, electrical and mechanical characterization of magnetron-sputtered V–Ge–C thin films , 2008 .

[13]  N. Schell,et al.  Phase stability of epitaxially grown Ti2AlN thin films , 2006 .

[14]  S. Mändl,et al.  Influence of nitrogen implantation on the high temperature oxidation of titanium-base alloys , 2006 .

[15]  Yanchun Zhou,et al.  Atomic scale characterization of layered ternary Cr2AlC ceramic , 2006 .

[16]  J. Emmerlich,et al.  Photoemission studies of Ti3SiC2 and nanocrystalline-TiC/amorphous-SiC nanocomposite thin films , 2006 .

[17]  Jinbang Wang,et al.  High-temperature oxidation and hot corrosion of Cr2AlC , 2007 .

[18]  Zhimei Sun,et al.  Effect of the Composition on the Structure of Cr‐Al‐C Investigated by Combinatorial Thin Film Synthesis and ab Initio Calculations , 2004 .

[19]  M. Akinc,et al.  Synthesis and high-temperature stability of Ti3SiC2 , 1999 .

[20]  W. Quadakkers,et al.  Oxidation-Resistant Aluminide Coatings on γ-TiAl , 2003 .

[21]  Yanchun Zhou,et al.  Oxidation behavior of Ti3AlC2 at 1000–1400 °C in air , 2003 .

[22]  J. Thornton High Rate Thick Film Growth , 1977 .

[23]  Ulf Jansson,et al.  The Mn+1AXn phases: Materials science and thin-film processing , 2010 .

[24]  L. Hultman,et al.  Single-crystal Ti2AlN thin films , 2005 .

[25]  S. W. Park,et al.  Oxidation of Cr2AlC Between 900 and 1200 °C in Air , 2007 .

[26]  V. Singh,et al.  Oxidation behaviour of the near α-titanium alloy IMI 834 , 2004 .

[27]  L. Hultman,et al.  Magnetron sputtering of Ti3SiC2 thin films from a Ti3SiC2 compound target , 2007 .

[28]  Yanfei Zhou,et al.  High-Temperature Oxidation Behavior of Ti2AlC in Air , 2003 .

[29]  J. Emmerlich,et al.  Thermal stability of Ti3SiC2 thin films , 2007 .

[30]  Zushu Hu,et al.  Oxidation Behavior of Graded NiCrAlYRe Coatings at 900, 1000 and 1100 °C , 2009 .

[31]  Guo‐Jun Zhang,et al.  Oxidation behavior of Cr2AlC ceramics at 1,100 and 1,250 °C , 2008 .

[32]  Yanchun Zhou,et al.  Recent Progress in Theoretical Prediction, Preparation, and Characterization of Layered Ternary Transition-Metal Carbides , 2009 .

[33]  J. Schneider,et al.  Towards large area deposition of Cr2AlC on steel , 2006 .

[34]  J. Emmerlich,et al.  Elastic properties of Cr2AlC thin films probed by nanoindentation and ab initio molecular dynamics , 2007 .

[35]  N. Schell,et al.  Nucleation and growth of Ti2AlN thin films deposited by reactive magnetron sputtering onto MgO(111) , 2007 .

[36]  Lars Hultman,et al.  Microstructural evolution during film growth , 2003 .