Propagation of shear bands in a Cu_47.5Zr_47.5Al_5 bulk metallic glass

We report a novel finding of slither propagation of shear bands on the fracture surface of a Cu_47.5Zr_47.5Al_5 bulk metallic glass (BMG). The nanoscale heterogeneities in the as-cast state are aggregated along shear bands with irregular morphology. Such heterogeneities create a fluctuating stress field during shear band propagation leading to a slither propagation mode. The slither propagation of 10 to 15 nm wide shear bands is effective to improve both the plasticity and the “work-hardening-like” behavior of BMGs if the size, the morphology, and the elastic properties of the heterogeneities are intimately intercalated during solidification.

[1]  J. Eckert,et al.  Work hardening ability of ductile Ti45Cu40Ni7.5Zr5Sn2.5 and Cu47.5Zr47.5Al5 bulk metallic glasses , 2006 .

[2]  K. B. Kim,et al.  Effect of Sn on microstructure and mechanical properties of (Ti–Cu)-based bulk metallic glasses , 2006 .

[3]  Rahul K Gupta,et al.  Rheological and Mechanical Comparative Study of In Situ Polymerized and Melt-Blended Nylon 6 Nanocomposites , 2005 .

[4]  W. Johnson,et al.  A universal criterion for plastic yielding of metallic glasses with a (T/Tg) 2/3 temperature dependence. , 2005, Physical review letters.

[5]  A. Inoue,et al.  Nanoscale multistep shear band formation by deformation-induced nanocrystallization in Zr-Al-Ni-Pd bulk metallic glass , 2005 .

[6]  J. Eckert,et al.  "Work-Hardenable" ductile bulk metallic glass. , 2005, Physical review letters.

[7]  A. Yavari,et al.  Unusual room-temperature compressive plasticity in nanocrystal-toughened bulk copper-zirconium glass , 2005 .

[8]  W. Wang,et al.  Fracture of brittle metallic glasses: brittleness or plasticity. , 2005, Physical review letters.

[9]  Yaohe Zhou,et al.  Mechanically driven phase separation and corresponding microhardness change in Cu60Zr20Ti20 bulk metallic glass , 2005 .

[10]  Weihua Wang,et al.  Intrinsic plasticity or brittleness of metallic glasses , 2005 .

[11]  Jan Schroers,et al.  Ductile bulk metallic glass. , 2004, Physical review letters.

[12]  A. Inoue,et al.  Influence of hydrostatic pressure during casting on as cast structure and mechanical properties in Zr65Al7.5Ni10Cu17.5-xPdx (x = 0, 17.5) alloys , 2004 .

[13]  Weihua Wang,et al.  Bulk metallic glasses , 2004 .

[14]  Jing Li,et al.  Nanometre-scale defects in shear bands in a metallic glass , 2002 .

[15]  K. T. Ramesh,et al.  Enhanced plastic strain in Zr-based bulk amorphous alloys , 2001 .

[16]  Akihisa Inoue,et al.  High-strength Cu-based bulk glassy alloys in Cu-Zr-Ti and Cu-Hf-Ti ternary systems , 2001 .

[17]  Daniel M. Mueth,et al.  Signatures of granular microstructure in dense shear flows , 2000, Nature.

[18]  S. D. Papka,et al.  Biaxial crushing of honeycombs: - Part 1: Experiments , 1999 .

[19]  W. Johnson Bulk Glass-Forming Metallic Alloys: Science and Technology , 1999 .

[20]  J. Harden,et al.  Inhomogeneous Flows of Complex Fluids: Mechanical Instability Versus Non-Equilibrium Phase Transition , 1997 .

[21]  W. Stobbs,et al.  The structure of shear bands in metallic glasses , 1981 .

[22]  Frans Spaepen,et al.  A microscopic mechanism for steady state inhomogeneous flow in metallic glasses , 1977 .

[23]  W. Xu,et al.  Ductile metallic glasses in supercooled martensitic alloys , 2006 .

[24]  A. Argon Mechanisms of inelastic deformation in metallic glasses , 1982 .

[25]  A. Argon Plastic deformation in metallic glasses , 1979 .