Kinetics and Mechanisms of Oxidation of 2D Woven C/SiC Composites: I, Experimental Approach

The oxidation behavior of a 2D woven C/SiC composite partly protected with a SiC seal coating and heat-treated (stabilized) at 1,600 C in inert gas has been investigated through an experimental approach based on thermogravimetric analyses and optical/electron microscopy. Results of the tests, performed under flowing oxygen, have shown that the oxidation behavior of the composite material in terms of oxidation kinetics and morphological evolutions is related to the presence of thermal microcracks in the seal coating as well as in the matrix. Three different temperature domains exist. At low temperatures ( 1,100 C), such diffusion mechanisms are limited by sealing of the microcracks by silica; therefore, the degradation of the composite remains superficial. The study of the oxidation behavior of (i) the heat-treated composite in a lower oxygen content environment (dry air) and (ii) themore » as-processed (unstabilized) composite in dry oxygen confirms the different mechanisms proposed to explain the oxidation behavior of the composite material.« less

[1]  R. Naslain,et al.  Kinetics and Mechanisms of Oxidation of 2D Woven C/SiC Composites: II, Theoretical Approach , 1994 .

[2]  X. Bourrat,et al.  Structure/oxidation behavior relationship in the carbonaceous constituents of 2D-C/PyC/SiC composites , 1993 .

[3]  C. Jaussaud,et al.  Oxidation kinetics of SiC deposited from CH3SiCl3/H2 under CVI conditions , 1992 .

[4]  R. Bhatt Oxidation Effects on the Mechanical Properties of a SiC-Fiber-Reinforced Reaction-Bonded Si3N4 Matrix Composite , 1992 .

[5]  R. E. Tressler,et al.  Oxidation of Single‐Crystal Silicon Carbide Part II . Kinetic Model , 1990 .

[6]  R. E. Tressler,et al.  Oxidation of Single‐Crystal Silicon Carbide Part I . Experimental Studies , 1990 .

[7]  N. Fréty,et al.  Relationship between high-temperature development of fibre-matrix interfaces and the mechanical behaviour of SiCSiC composites , 1990 .

[8]  J. Cavalier,et al.  Composites a Matrice Ceramique, Nouveaux Materiaux a Tres Hautes Performances , 1989 .

[9]  K. Prewo,et al.  The oxidative stability of carbon fibre reinforced glass-matrix composites , 1988 .

[10]  J. Sheehan,et al.  Ceramic coatings for carbon-carbon composites , 1988 .

[11]  K. Luthra Oxidation of carbon/carbon composites—a theoretical analysis , 1988 .

[12]  S. Marinkovic,et al.  Kinetics of air oxidation of unidirectional carbon fibres/ CVD carbon composites , 1987 .

[13]  D. Mckee Oxidation behavior and protection of carbon/carbon composites , 1987 .

[14]  P. Hagenmuller,et al.  Synthesis and properties of new composite materials for high temperature applications based on carbon fibers and C-SiC or C-TiC hybrid matrices. , 1981 .