INTERACTION OF HISTORICAL LEAD GLAZES WITH CORROSIVE MEDIA

*Department of Glass and Ceramics, University of Chemistry and Technology Prague, Technická 5, 166 28 Prague 6, Czech Republic **Laboratory of Inorganic Materials, University of Chemistry and Technology Prague, Technická 5, 166 28, Prague 6, Czech Republic ***Institute of Rock Structure and Mechanics of the Czech Academy of Sciences, V Holešovičkách 41, 182 09, Prague 8, Czech Republic ****Central Laboratories, University of Chemistry and Technology Prague, Technická 5, 166 28 Prague 6, Czech Republic

[1]  P. Ausset,et al.  Alteration rate of medieval potash-lime silicate glass as a function of pH and temperature: A low pH-dependent dissolution , 2020 .

[2]  S. Narayanasamy,et al.  Glass alteration in atmospheric conditions: crossing perspectives from cultural heritage, glass industry, and nuclear waste management , 2020, npj Materials Degradation.

[3]  L. Hupa,et al.  The impact of wollastonite and dolomite on chemical durability of matte fast-fired raw glazes , 2020 .

[4]  M. Kolarova,et al.  Thermal behaviour of glazed ceramic bodies , 2020, Journal of Thermal Analysis and Calorimetry.

[5]  P. Dvořáková,et al.  Multi-methodical study of Early Modern Age archaeological glazed ceramics from Prague , 2020, Heritage Science.

[6]  F. M. Ezz-eldin,et al.  Influence of Industrial Solid Waste on the Chemical and Mechanical Properties of Traditional Glaze-Ceramics , 2018, Silicon.

[7]  T. Charpentier,et al.  New insight into atmospheric alteration of alkali-lime silicate glasses , 2017 .

[8]  S. Gin,et al.  Structure and Chemical Durability of Lead Crystal Glass. , 2016, Environmental science & technology.

[9]  Fei Wang,et al.  The role of firing process on bubble formation in a glaze layer of sanitary ware , 2014 .

[10]  M. Grilc,et al.  An integrated experimental-modeling approach to study the acid leaching behavior of lead from sub-micrometer lead silicate glass particles. , 2013, Journal of hazardous materials.

[11]  K. Mueller,et al.  An international initiative on long-term behavior of high-level nuclear waste glass , 2013 .

[12]  C. Watt,et al.  Acetic and formic acids emitted from wood samples and their effect on selected materials in museum environments , 2010 .

[13]  J. Tate,et al.  Alteration of soda silicate glasses by organic pollutants in museums: Mechanisms and kinetics , 2009 .

[14]  A. Hamidi,et al.  Hydrolysis kinetics of lead silicate glass in acid solution , 2009 .

[15]  Philippe Barboux,et al.  On the effect of glass composition in the dissolution of glasses by water , 2008 .

[16]  V. Ducman,et al.  Low-vacuum SEM analyses of ceramic tiles with emphasis on glaze defects characterisation , 2007 .

[17]  L. Hupa,et al.  Chemical durability of glazed surfaces , 2007 .

[18]  A. Sjöberg,et al.  Chemical resistance and cleanability of glazed surfaces , 2005 .

[19]  R. Bertoncello,et al.  Leaching of lead silicate glasses in acid environment: compositional and structural changes , 2004 .

[20]  S. Turrell,et al.  Alteration of lead silicate glasses due to leaching in heated acid solutions , 2003 .

[21]  A. Doménech‐Carbó,et al.  Voltammetric Identification of Lead(II) and (IV) in Mediaeval Glazes in Abrasion‐Modified Carbon Paste and Polymer Film Electrodes. Application to the Study of Alterations in Archaeological Ceramic , 2000 .

[22]  F. Fayon,et al.  29Si and 207Pb NMR study of local order in lead silicate glasses , 1998 .

[23]  Paul W. Wang,et al.  Structural role of lead in lead silicate glasses derived from XPS spectra , 1996 .

[24]  W. Ebert The effects of the glass surface area/solution volume ratio on glass corrosion: A critical review , 1995 .

[25]  D. Clark,et al.  Corrosion of Glass, Ceramics and Ceramic Superconductors: Principles, Testing, Characterization and Applications , 1993 .

[26]  A. Helebrant,et al.  A mathematical model used to compare glass durability tests under different flow conditions , 1989 .

[27]  C. Byers,et al.  Aqueous corrosion of natural and nuclear waste glasses I. Comparative rates of hydration in liquid and vapor environments at elevated temperatures , 1986 .

[28]  S. Wood,et al.  Corrosion of Lead Glasses in Acid Media: I, Leaching Kinetics , 1978 .