Variation of optical properties of gel-derived VO2 thin films with temperature

VO2 thin films are prepared on three kinds of substrates by the sol-gel dip-coating method followed by heat treatment under vacuum conditions. The IR and UV-visible spectra of the films are studied during heating and cooling between room temperature and 100 degree(s)C. The experimental results show that the films exhibit thermally-induced reversible phase transition and, as a result, the maximum changes in transmittance and reflectivity are 58% and 25%, respectively, in the case of vacuum heat treatment at 400 degree(s)C and silica glass substrates. The refractive index n decreases and the extinction coefficient k increases when heating these films from room temperature to 100 degree(s)C, and vice versa. The reasons why the optical constants and IR absorption spectra change so remarkably are discussed.