Experimental Investigation on Hybrid Friction Stir Processing using compressed air in Aluminum 7075 alloy
暂无分享,去创建一个
V. Badheka | U. Patel | Vivek V. Patel | Sagar R. Patel | Swarg N. Patel | Samarth R. Zala | Kedar Badheka
[1] Abhishek Kumar,et al. Influence of Friction Stir Processed Parameters on Superplasticity of Al-Zn-Mg-Cu Alloy , 2016 .
[2] C. Cepeda-Jiménez,et al. Lowering the temperature for high strain rate superplasticity in an Al-Mg-Zn-Cu alloy via cooled friction stir processing , 2013 .
[3] Z. Ma,et al. Achieving high strain rate superplasticity in cast 7075Al alloy via friction stir processing , 2009, Journal of Materials Science.
[4] K. Sreekumar,et al. Metallurgical Studies on Cracked Al–5.5Zn–2.5Mg–1.5Cu Aluminum Alloy Injector Disc of Turbine Rotor , 2008 .
[5] Rajiv S. Mishra,et al. Superplastic deformation behaviour of friction stir processed 7075Al alloy , 2002 .
[6] A. Mukherjee,et al. High Strain Rate Superplasticity in a Friction Stir Processed 7075 Al Alloy , 1999 .
[7] Abhishek Kumar,et al. Effect of Velocity Index on Grain Size of Friction Stir Processed Al-Zn-Mg-Cu Alloy , 2016 .
[8] S. Karabay,et al. Influence of Different Heat Treatments on the Solid Particle Erosion Behavior of Aluminum Alloy AA 7075 in Industrial Applications , 2015 .
[9] Z. Ma,et al. Effects of heating rates on microstructure and superplastic behavior of friction stir processed 7075 aluminum alloy , 2014, Journal of Materials Science.
[10] H. Svoboda,et al. Superplasticity of a Friction Stir Processed 7075-T651 Aluminum Alloy , 2012 .
[11] R. K. Gupta,et al. Investigation of internal cracks in aluminium alloy AA7075 forging , 2006 .