Characterisation of pre-industrial hybrid cement and effect of pre-curing temperature
暂无分享,去创建一个
Ángel Palomo | Jose Ygnacio Pastor | Ana Fernández-Jiménez | B. Qu | A. Fernández-Jiménez | J. Y. Pastor | A. Martín | Bo Qu | A. Palomo | A. Martin | J. Pastor
[1] B. Lothenbach,et al. Chemical activation of hybrid binders based on siliceous fly ash and Portland cement , 2016 .
[2] M. Zając,et al. Hydration of quaternary Portland cement blends containing blast-furnace slag, siliceous fly ash and limestone powder , 2015 .
[3] Ángel Palomo,et al. A review on alkaline activation: new analytical perspectives , 2014 .
[4] Ángel Palomo,et al. The Early Age Hydration Reactions of a Hybrid Cement Containing a Very High Content of Coal Bottom Ash , 2014 .
[5] Sagrario Martínez-Ramírez,et al. FTIR study of the effect of temperature and nanosilica on the nano structure of C–S–H gel formed by hydrating tricalcium silicate , 2014 .
[6] Ángel Palomo,et al. Variation in hybrid cements over time. Alkaline activation of fly ash–portland cement blends , 2013 .
[7] Ángel Palomo,et al. Hydration kinetics in hybrid binders: Early reaction stages , 2013 .
[8] Obada Kayali,et al. Assessment of high volume replacement fly ash concrete – Concept of performance index , 2013 .
[9] John L. Provis,et al. Engineering and durability properties of concretes based on alkali-activated granulated blast furnac , 2012 .
[10] Á. G. Torre,et al. Rietveld Quantitative Phase Analysis of OPC Clinkers, Cements and Hydration Products , 2012 .
[11] B. Lothenbach,et al. Supplementary cementitious materials , 2011 .
[12] Á. Palomo,et al. Compatibility studies between N-A-S-H and C-A-S-H gels. Study in the ternary diagram Na2O–CaO–Al2O3–SiO2–H2O , 2011 .
[13] Martin Schneider,et al. Sustainable cement production—present and future , 2011 .
[14] C. Shi,et al. New cements for the 21st century: The pursuit of an alternative to Portland cement , 2011 .
[15] Dale P. Bentz,et al. Evaluation of Sustainable High-Volume Fly Ash Concretes | NIST , 2011 .
[16] Á. Palomo,et al. Alkali activation of fly ash. Part III: Effect of curing conditions on reaction and its graphical description , 2010 .
[17] J. Sharp,et al. Variation in the Composition of C‐S‐H Gel in Portland Cement Pastes Cured at Various Temperatures , 2004 .
[18] Á. Palomo,et al. Alkaline Activation of Fly Ashes: NMR Study of the Reaction Products , 2004 .
[19] Jeffrey J. Thomas,et al. Effect of hydration temperature on the solubility behavior of Ca-, S-, Al-, and Si-bearing solid phases in Portland cement pastes , 2003 .
[20] F. Puertas,et al. Structure of Calcium Silicate Hydrates Formed in Alkaline-Activated Slag: Influence of the Type of Alkaline Activator , 2003 .
[21] M. Collepardi,et al. A state-of-the-art review on delayed ettringite attack on concrete , 2003 .
[22] C. Shi,et al. Alkali-Activated Cements and Concretes , 2003 .
[23] H. J. Jakobsen,et al. Incorporation of aluminum in the calcium silicate hydrate (C-S-H) of hydrated portland cements: a high-field 27Al and 29Si MAS NMR investigation. , 2003, Inorganic chemistry.
[24] H. Panepucci,et al. 29Si and 27Al high-resolution NMR characterization of calcium silicate hydrate phases in activated blast-furnace slag pastes , 2001 .
[25] J. Sharp,et al. The microstructure and mechanical properties of blended cements hydrated at various temperatures , 2001 .
[26] John H. Sharp,et al. The effect of temperature on the early hydration of Portland cement and blended cements , 2000 .
[27] Francisca Puertas,et al. Alkali-activated slag mortars: Mechanical strength behaviour , 1999 .
[28] I. Richardson,et al. The structure of the calcium silicate hydrate phases present in hardened pastes of white Portland cement/blast-furnace slag blends , 1997 .
[29] Caijun Shi,et al. A calorimetric study of early hydration of alkali-slag cements , 1995 .
[30] Karen Scrivener,et al. Delayed ettringite formation , 2001 .
[31] P. L. Pratt,et al. Factors affecting the strength of alkali-activated slag , 1994 .
[32] J. Beaudoin,et al. Effect of temperature on sulphate adsorption/desorption by tricalcium silicate hydrates , 1994 .
[33] J. Young,et al. Silicate polymerization during the hydration of alite , 1983 .