Effect of pressure on corrosion behavior of X60, X65, X70, and X80 carbon steels in water-unsaturated supercritical CO2 environments

[1]  A. Neville,et al.  The effect of O 2 content on the corrosion behaviour of X65 and 5Cr in water-containing supercritical CO 2 environments , 2015 .

[2]  A. Neville,et al.  The influence of SO2 on the tolerable water content to avoid pipeline corrosion during the transportation of supercritical CO2 , 2015 .

[3]  A. Neville,et al.  Understanding the Influence of SO2 and O2 on the Corrosion of Carbon Steel in Water-Saturated Supercritical CO2 , 2015 .

[4]  A. Neville,et al.  Relating iron carbonate morphology to corrosion characteristics for water-saturated supercritical CO2 systems , 2015 .

[5]  A. Neville,et al.  Comparison of corrosion behaviour for X-65 carbon steel in supercritical CO2-saturated water and water-saturated/unsaturated supercritical CO2 , 2015 .

[6]  A. Neville,et al.  Effect of temperature on the critical water content for general and localised corrosion of X65 carbon steel in the transport of supercritical CO2 , 2014 .

[7]  Ivan S. Cole,et al.  Investigating the Effect of Water Content in Supercritical CO2 as Relevant to the Corrosion of Carbon Capture and Storage Pipelines , 2014 .

[8]  S. Nešić,et al.  Corrosion Behavior of Deep Water Oil Production Tubing Material Under Supercritical CO2 Environment: Part 1—Effect of Pressure and Temperature , 2014 .

[9]  W. Ni,et al.  A mechanistic model for pipeline steel corrosion in supercritical CO2–SO2–O2–H2O environments , 2013 .

[10]  Ranjith Pathegama Gamage,et al.  Investigating the effect of salt and acid impurities in supercritical CO2 as relevant to the corrosion of carbon capture and storage pipelines , 2013 .

[11]  Z. Wang,et al.  Long term corrosion of X70 steel and iron in humid supercritical CO2 with SO2 and O2 impurities , 2013 .

[12]  Z. Wang,et al.  Effect of temperature on corrosion behaviour of X70 steel in high pressure CO2/SO2/O2/H2O environments , 2013 .

[13]  Zhe Wang,et al.  Effect of Exposure Time on the Corrosion Rates of X70 Steel in Supercritical CO2/SO2/O2/H2O Environments , 2013 .

[14]  Aki Sebastian Ruhl,et al.  Investigation of corrosive effects of sulphur dioxide, oxygen and water vapour on pipeline steels , 2013 .

[15]  S. Nešić,et al.  CO2 Top-of-the-Line Corrosion in Presence of Acetic Acid: A Parametric Study , 2013 .

[16]  Weidou Ni,et al.  The upper limit of moisture content for supercritical CO2 pipeline transport , 2012 .

[17]  Xin Li,et al.  Discussion of the CO2 corrosion mechanism between low partial pressure and supercritical condition , 2012 .

[18]  Chao Xu,et al.  Impact of SO2 concentration on the corrosion rate of X70 steel and iron in water-saturated supercritical CO2 mixed with SO2 , 2011 .

[19]  Yoon-Seok Choi,et al.  Determining the corrosive potential of CO2 transport pipeline in high pCO2-water environments , 2011 .

[20]  D. Bettge,et al.  The challenge in understanding the corrosion mechanisms under oxyfuel combustion conditions , 2011 .

[21]  Yoon-Seok Choi,et al.  Effect of impurities on the corrosion behavior of CO2 transmission pipeline steel in supercritical CO2-water environments. , 2010, Environmental science & technology.

[22]  M. Mølnvik,et al.  Dynamis CO2 quality recommendations , 2008 .

[23]  Chi Hong Chio,et al.  The hydrates and deuterates of ferrous sulfate (FeSO4): a Raman spectroscopic study , 2007 .

[24]  Zaoxiao Zhang,et al.  Optimization of pipeline transport for CO2 sequestration , 2006 .

[25]  John Gale,et al.  Transmission of CO2-Safety and Economic Considerations , 2004 .

[26]  R. Nishimura,et al.  Hydrogen permeation and corrosion behavior of high strength steel MCM 430 in cyclic wet–dry SO2 environment , 2004 .

[27]  Karsten Pruess,et al.  CO2-H2O mixtures in the geological sequestration of CO2. I. Assessment and calculation of mutual solubilities from 12 to 100°C and up to 600 bar , 2003 .