Micro-Raman study of the fatigue and fracture behaviour of single PA66 fibres: Comparison with single PET and PP fibres
暂无分享,去创建一个
P. Colomban | A. Marcellan | A. Bunsell | R. Paquin | J. Ramírez | Philippe Colomban | José Martin Herrera Ramirez | Raphael Paquin | Alba | Marcellan