Correlating Metal Poisoning with Zeolite Deactivation in an Individual Catalyst Particle by Chemical and Phase-Sensitive X-ray Microscopy

Fluid catalytic cracking (FCC) is the main conversion process used in oil refineries. An X-ray microscopy method is used to show that metal poisoning and related structural changes in the zeolite active material lead to a non-uniform core–shell deactivation of FCC catalyst particles. The study links the detrimental effect of V and Ni poisoning with zeolite destruction and dealumination in a spatial manner within a single FCC catalyst particle.

[1]  S. Voutetakis,et al.  Effect of metals poisoning on FCC products yields: studies in an FCC short contact time pilot plant unit , 2001 .

[2]  Bert M. Weckhuysen,et al.  Heterogeneities of individual catalyst particles in space and time as monitored by spectroscopy. , 2012, Nature chemistry.

[3]  B. Weckhuysen,et al.  Microspectroscopic insight into the deactivation process of individual cracking catalyst particles with basic sulfur components , 2012 .

[4]  A. Beale,et al.  Combined experimental and computational modelling studies of the solubility of nickel in strontium titanate , 2009 .

[5]  J. Spivey,et al.  Structural Characterization of Ni-Substituted Hexaaluminate Catalysts Using EXAFS, XANES, XPS, XRD, and TPR , 2010 .

[6]  Hui Cao,et al.  Spectroscopic Studies of the Migration of Vanadium in the Model Fluid Catalytic Cracking Process , 1995 .

[7]  B. Weckhuysen,et al.  Catalytic activity in individual cracking catalyst particles imaged throughout different life stages by selective staining. , 2011, Nature chemistry.

[8]  B. Weckhuysen,et al.  Staining of fluid-catalytic-cracking catalysts: localising Brønsted acidity within a single catalyst particle. , 2012, Chemistry.

[9]  J. Susini,et al.  New methodological approach for the vanadium K-edge X-ray absorption near-edge structure interpretation: application to the speciation of vanadium in oxide phases from steel slag. , 2007, The journal of physical chemistry. B.

[10]  B. Weckhuysen Chemical imaging of spatial heterogeneities in catalytic solids at different length and time scales. , 2009, Angewandte Chemie.

[11]  K. Chao,et al.  Vanadium passivation of cracking catalysts by imaging secondary ion mass spectrometry , 1995 .

[12]  Christian G. Schroer,et al.  Hard and soft X-ray microscopy and tomography in catalysis: bridging the different time and length scales. , 2010, Chemical Society reviews.

[13]  A. Psarras,et al.  Study of the accessibility effect on the irreversible deactivation of FCC catalysts from contaminant feed metals , 2007 .

[14]  P. Jacobs,et al.  The Mechanism of Zeolite Y Destruction by Steam in the Presence of Vanadium , 1997 .

[15]  Yung Ngothai,et al.  Probing ore deposits formation: New insights and challenges from synchrotron and neutron studies , 2010 .

[16]  J. Newsam The Zeolite Cage Structure , 1986, Science.

[17]  W. Vermeiren,et al.  Impact of Zeolites on the Petroleum and Petrochemical Industry , 2009 .

[18]  Xinsheng Liu,et al.  Pathways for Y Zeolite Destruction: The Role of Sodium and Vanadium , 2002 .

[19]  Taha Sochi,et al.  Dynamic X-ray diffraction computed tomography reveals real-time insight into catalyst active phase evolution. , 2011, Angewandte Chemie.

[20]  E. Scavetta,et al.  Combined Use of Synchrotron‐Radiation‐Based Imaging Techniques for the Characterization of Structured Catalysts , 2010 .

[21]  C. Marshall,et al.  29Si and 27Al n.m.r. study of steamed faujasites: evidence for non-framework tetrahedrally bound aluminium , 1987 .

[22]  Bert M. Weckhuysen,et al.  Active phase evolution in single Ni/Al2O3 methanation catalyst bodies studied in real time using combined μ-XRD-CT and μ-absorption-CT , 2012 .

[23]  M. Ryan,et al.  In situ determination of the nickel oxidation state in La2NiO4+δ and La4Ni3O10−δ using X-ray absorption near-edge structure , 2011 .

[24]  M. M. Pereira,et al.  Role of nickel and vanadium over USY and RE-USY coke formation , 2006 .

[25]  Bert M. Weckhuysen Chemische Bildgebung von räumlichen Heterogenitäten in katalytischen Festkörpern auf unterschiedlichen Längen‐ und Zeitskalen , 2009 .

[26]  P. Bleuet,et al.  Probing the structure of heterogeneous diluted materials by diffraction tomography. , 2008, Nature materials.

[27]  A. Beale,et al.  Chemical imaging of catalytic solids with synchrotron radiation. , 2010, Chemical Society reviews.

[28]  C. Fahrni,et al.  Biological applications of X-ray fluorescence microscopy: exploring the subcellular topography and speciation of transition metals. , 2007, Current opinion in chemical biology.

[29]  E. L. Kugler,et al.  Nickel and vanadium on equilibrium cracking catalysts by imaging secondary ion mass spectrometry , 1988 .

[30]  Jean Susini,et al.  Blackening of Pompeian cinnabar paintings: X-ray microspectroscopy analysis. , 2006, Analytical chemistry.

[31]  Avelino Corma,et al.  Inorganic Solid Acids and Their Use in Acid-Catalyzed Hydrocarbon Reactions , 1995 .