Microstructure and anti-oxidation properties of Yb2Si2O7/SiC bilayer coating for C/SiC composites
暂无分享,去创建一个
Yang Li | Zhuan Li | P. Xiao | L. Pan | Jin-wei Li | Dongmei Pu | Pengju Chen | L. Pang | Liang Pang
[1] Yang Li,et al. Microstructure and oxidation behavior of a novel bilayer (c-AlPO4–SiCw–mullite)/SiC coating for carbon fiber reinforced CMCs , 2019, Journal of the European Ceramic Society.
[2] K. Rezwan,et al. Damage analysis of 2.5D C/C-SiC composites subjected to fatigue loadings , 2019, Journal of the European Ceramic Society.
[3] Yang Li,et al. Mechanical response and microstructure of 2D carbon fiber reinforced CMCs containing Cu-Si alloy exposed to fatigue stresses , 2019, Composites Part B: Engineering.
[4] W. Zhou,et al. Microstructural evolution of SiC coating on C/C composites exposed to 1500 °C in ambient air , 2019, Ceramics International.
[5] Y. Long,et al. Mechanical properties of CVD-SiC coatings with Si impurity , 2018, Ceramics International.
[6] Yan Jiang,et al. Microstructure and oxidation behaviors of dense mullite‑silicon carbide‑silicon coating for graphite fabricated by dipping-pyrolysis and reactive infiltration , 2018, Surface and Coatings Technology.
[7] Yang Li,et al. LPCVD-based SiO 2 /SiC multi-layers coating on graphite for improved anti-oxidation at wide-ranged temperatures , 2018, Composites Part B: Engineering.
[8] Y. Xiang,et al. Mullite whisker toughened mullite coating to enhance the thermal shock resistance of SiC pre-coated carbon/carbon composites , 2017 .
[9] Liping Huang,et al. Relationship between cracks and microstructures in APS YSZ coatings at elevated temperatures , 2017 .
[10] L. Su,et al. Effects of CMAS penetration on the delamination cracks in EB-PVD thermal barrier coatings with curved interface , 2017 .
[11] Ying Wang,et al. Microstructure and oxidation resistant behavior of Er2Si2O7 and Er2Si2O7/LaMgAl11O19 coatings deposited on Cf/SiC composites by APS at 1723 K , 2017 .
[12] Ying Wang,et al. Oxidation and thermal shock resistant properties of Si/Yb2SiO5/NdMgAl11O19 coating deposited on Cf/SiC composites , 2017 .
[13] Zhuan Li,et al. Oxidation behavior of C/C composites with SiC/ZrSiO 4 –SiO 2 coating , 2017 .
[14] Chenglong Hu,et al. Design, Preparation and Properties of Carbon Fiber Reinforced Ultra-High Temperature Ceramic Composites for Aerospace Applications: A Review , 2017 .
[15] W. Krenkel,et al. Fatigue behavior and residual strength evolution of 2.5D C/C-SiC composites , 2016 .
[16] Jianfeng Huang,et al. A mullite oxidation protective coating on SiC coated carbon/carbon composites by hot dipping , 2016 .
[17] W. Krenkel,et al. Strength evolution of cyclic loaded LSI-based C/C-SiC composites , 2016 .
[18] Yu Xiaoyu,et al. Thermal cycling behavior and oxidation resistance of SiC whisker-toughened-mullite/SiC coated carbon/carbon composites in burner rig tests , 2016 .
[19] H. Wadley,et al. Response of ytterbium disilicate–silicon environmental barrier coatings to thermal cycling in water vapor , 2016 .
[20] Peter Kenesei,et al. The influence of calcium–magnesium–aluminosilicate deposits on internal stresses in Yb 2 Si 2 O 7 multilayer environmental barrier coatings , 2016 .
[21] Yu Xiaoyu,et al. Microstructure and oxidation behavior of sol–gel mullite coating on SiC-coated carbon/carbon composites , 2015 .
[22] Hejun Li,et al. Effect of pre-oxidation on the ablation resistance of ZrB2–SiC coating for SiC-coated carbon/carbon composites , 2015 .
[23] Lai-fei Cheng,et al. Structure design and fabrication of environmental barrier coatings for crack resistance , 2014 .
[24] Yanchun Zhou,et al. Synthesis and characterization of β-Yb2Si2O7 powders , 2013 .
[25] Xizhi Fan,et al. A new double layer oxidation resistant coating based on Er2SiO5/LaMgAl11O19 deposited on C/SiC composites by atmospheric plasma spraying , 2013 .
[26] Jianfeng Huang,et al. Microstructure and oxidation resistance of C-AlPO4–mullite coating prepared by hydrothermal electrophoretic deposition for SiCC/C composites , 2013 .
[27] Jianfeng Huang,et al. A mullite/SiC oxidation protective coating for carbon/carbon composites , 2013 .
[28] E. Opila,et al. Oxidation of Carbon Fiber‐Reinforced Silicon Carbide Matrix Composites at Reduced Oxygen Partial Pressures , 2011 .
[29] Hejun Li,et al. A Si–Mo–W Coating to Protect SiC-Coated Carbon/Carbon Composites Against Oxidation , 2009 .
[30] Yiguang Wang,et al. First-principles investigation on the corrosion resistance of rare earth disilicates in water vapor , 2009 .
[31] K. Nickel,et al. High temperature water vapour corrosion of rare earth disilicates (Y,Yb,Lu)2Si2O7 in the presence of Al(OH)3 impurities , 2007 .
[32] V. Sarin,et al. The development of CVD mullite coatings for high temperature corrosive applications , 1997 .