Structural-Phase State and Properties of Cr-Al-Si-N Coatings Obtained by Vacuum Arc Plasma Deposition

[1]  M. Boiko,et al.  Investigation of changes in the properties of diamond-like films under friction by the XPS method , 2021, Journal of Physics: Conference Series.

[2]  V. Kolesnikov,et al.  The performance evaluation of heavy loaded tribosystems with vacuum ion-plasma PVD and DLC coatings , 2021, Journal of Physics: Conference Series.

[3]  E. Novikov,et al.  Effect of the Adhesive Properties of Vacuum Ion-Plasma TiAlN Coatings on Wear Resistance in Friction , 2021, Journal of Friction and Wear.

[4]  O. V. Kudryakov,et al.  Effective Wear Resistance Parameters of Ion-Plasma Tribological Coatings , 2021, Defect and Diffusion Forum.

[5]  O. V. Kudryakov,et al.  Structural Aspects of Wear Resistance of Coatings Deposited by Physical Vapor Deposition , 2020, Physical Mesomechanics.

[6]  D. Kovacheva,et al.  Mechanical and Structural Properties of Nanocomposite CrAlSiN–AlSiN Coating with Periodically Modulated Composition , 2020, Coatings.

[7]  O. V. Kudryakov,et al.  Conditions and mechanisms of the defects formation in vacuum ion-plasma coatings , 2019, IOP Conference Series: Materials Science and Engineering.

[8]  Fan Qixiang,et al.  Microstructure and Properties of CrAlSiN Coatings Deposited by HiPIMS and Direct-Current Magnetron Sputtering , 2019, Coatings.

[9]  A. V. Sidashov,et al.  Nonequilibrium processes of segregation and diffusion in metal-polymer tribosystems , 2017 .

[10]  J. Yun,et al.  Microstructure, Mechanical, Oxidation and Corrosion Properties of the Cr-Al-Si-N Coatings Deposited by a Hybrid Sputtering System , 2017 .

[11]  Li Chen,et al.  Interfacial structure, mechanical properties and thermal stability of CrAlSiN/CrAlN multilayer coatings , 2017 .

[12]  A. Kozakov,et al.  Auger and X-Ray Photoelectron Spectroscopy Study of the Tribocontact Surface after Laser Modification , 2016 .

[13]  J. Duh,et al.  Development of Si-modified CrAlSiN nanocomposite coating for anti-wear application in extreme environment , 2015 .

[14]  V. Varavka,et al.  Integrated indentation tests of metal-ceramic nanocomposite coatings , 2015, Inorganic Materials.

[15]  Shubao Yang,et al.  Design of AlCrSiN multilayers and nanocomposite coating for HSS cutting tools , 2015 .

[16]  J. Duh,et al.  Influence of Si contents on tribological characteristics of CrAlSiN nanocomposite coatings , 2015 .

[17]  С. П. Буркин,et al.  АНАЛИЗ АДГЕЗИОННОГО ВЗАИМОДЕЙСТВИЯВ СИСТЕМЕ КАРБИД (ОКСИД, НИТРИД) – МЕТАЛЛЫ ГРУППЫ ЖЕЛЕЗА , 2015 .

[18]  Yin-Yu Chang,et al.  Wear behavior and cutting performance of CrAlSiN and TiAlSiN hard coatings on cemented carbide cutting tools for Ti alloys , 2014 .

[19]  C. Mitterer,et al.  Influence of Al and Si content on structure and mechanical properties of arc evaporated Al-Cr-Si-N thin films , 2013 .

[20]  E. Koumoulos,et al.  Nanotribological Behavior of Carbon Based Thin Films: Friction and Lubricity Mechanisms at the Nanoscale , 2013 .

[21]  Shihong Zhang,et al.  A superhard CrAlSiN superlattice coating deposited by multi-arc ion plating: I. Microstructure and mechanical properties , 2013 .

[22]  D. Jianxin,et al.  Friction and wear properties of TiN, TiAlN, AlTiN and CrAlN PVD nitride coatings , 2012 .

[23]  Z. Kou,et al.  Effect of removing internal residual metallic phases on wear resistance of polycrystalline diamond compacts , 2012 .

[24]  J. Duh,et al.  Oxidation resistance of nanocomposite CrAlSiN under long-time heat treatment , 2011 .

[25]  T. Polcar,et al.  High-temperature tribological properties of CrAlN, CrAlSiN and AlCrSiN coatings , 2011 .

[26]  Nick Bierwisch,et al.  Optimization of the Scratch Test for specific coating designs , 2011 .

[27]  V. Kolesnikov,et al.  Composition of an oxide layer formed by laser radiation and the structure of an oxide-metal interface on the surface of 9XC and P6M5 tool steels according to XPS , 2011 .

[28]  J. Duh,et al.  Oxidation behavior of Si-doped nanocomposite CrAlSiN coatings , 2010 .

[29]  A. Anders A structure zone diagram including plasma based deposition and ion etching - eScholarship , 2010 .

[30]  Chengyong Wang,et al.  Microstructure and properties of TiAlSiN coatings prepared by hybrid PVD technology , 2009 .

[31]  V. Kolesnikov,et al.  Study of the segregation processes and chemical bonding at equilibrium and nonequilibrium oxidation of the R6M5 alloy surface , 2009 .

[32]  T. Cho,et al.  Optimization of the Adhesion Strength of Arc Ion Plating TiAlN Films by the Taguchi Method , 2009, Materials.

[33]  Sheng-Min Yang,et al.  High temperature oxidation resistance of CrAlSiN coatings synthesized by a cathodic arc deposition process , 2008 .

[34]  Jože Vižintin,et al.  Tribological properties of DLC coatings and comparison with test results: Development of a database , 2008 .

[35]  K. Kim,et al.  Microstructures, mechanical properties, and tribological behaviors of Cr–Al–N, Cr–Si–N, and Cr–Al–Si–N coatings by a hybrid coating system , 2007 .

[36]  J. Zemek,et al.  XAES and XPS study of amorphous carbon nitride layers , 1998 .

[37]  G. Pharr,et al.  An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments , 1992 .

[38]  Nikolaos Michailidis,et al.  Nanoindentation , 2019, CIRP Encyclopedia of Production Engineering.