Evolution of microstructure and texture in grain-oriented 6.5%Si steel processed by strip-casting
暂无分享,去创建一个
R. Misra | Yandong Wang | G. Yuan | Xiang Lu | Yuanxiang Zhang | Yunbo Xu | F. Fang | Cao Guangming | Wang Guanqi
[1] G. Yuan,et al. Microstructure, texture and precipitate of grain-oriented 4.5 wt% Si steel by strip casting , 2016 .
[2] W. Mao,et al. Secondary Recrystallization Behaviors of Grain-Oriented 6.5 wt% Silicon Steel Sheets Produced by Rolling and Nitriding Processes , 2016, Acta Metallurgica Sinica (English Letters).
[3] T. Hiratani,et al. Magnetic Properties of Grain-oriented 6.5% Silicon Steel , 2016 .
[4] 智幸 大久保,et al. 一方向性6.5%けい素鋼板の磁気特性 , 2016 .
[5] Guodong Wang,et al. Effect of cooling rate on bending behavior of 6.5 wt.% Si electrical steel thin sheets fabricated by strip casting and rolling , 2016 .
[6] W. Mao,et al. Effect of texture and grain size on the magnetic flux density and core loss of cold-rolled high silicon steel sheets , 2015 .
[7] O. Perevertov,et al. Effect of applied tensile stress on the hysteresis curve and magnetic domain structure of grain-oriented transverse Fe-3%Si steel , 2015 .
[8] Hai‐Tao Liu,et al. Development of microstructure and texture in strip casting grain oriented silicon steel , 2015 .
[9] Hai‐Tao Liu,et al. Fabrication of grain-oriented silicon steel by a novel way: Strip casting process , 2014 .
[10] Jongryoul Kim,et al. Influence of cooling rate on iron loss behavior in 6.5 wt% grain-oriented silicon steel , 2014 .
[11] Zhen-Yu Liu,et al. Characterization of microstructure, texture and magnetic properties in twin-roll casting high silicon non-oriented electrical steel , 2014 .
[12] Jongryoul Kim,et al. Effect of ${\rm D}0_{3}$ Ordered Phase on Total Loss of 6.5 wt% Grain-Oriented Silicon Steel , 2012, IEEE Transactions on Magnetics.
[13] Hai‐Tao Liu,et al. Microstructure, texture and magnetic properties of strip-cast 1.3% Si non-oriented electrical steels , 2012 .
[14] Jongryoul Kim,et al. Influence of Low Temperature Heat Treatment on Iron Loss Behaviors of 6.5 wt% Grain-oriented Silicon Steels , 2012 .
[15] Jongryoul Kim,et al. Effects of Anti-phase Boundary on the Iron Loss of Grain Oriented Silicon Steel , 2011 .
[16] Huadong Fu,et al. Strain-softening behavior of an Fe–6.5 wt%Si alloy during warm deformation and its applications , 2011 .
[17] M. Imafuku,et al. Effects of laser irradiation on iron loss reduction for Fe–3%Si grain-oriented silicon steel , 2005 .
[18] A. Hunter,et al. Evolution of microstructure and texture during casting of AISI 304 stainless steel strip , 2002 .
[19] M. Komatsubara,et al. Newly developed electrical steel for high-frequency use , 2002 .
[20] K. Oh,et al. The Effects of Superheating on Texture and Microstructure of Fe–4.5wt%Si Steel Strip by Twin-roll Strip Casting , 2001 .
[21] K. Oh,et al. Microstructure and crystallographic texture of strip-cast 4.3wt%Si steel sheet , 1999 .
[22] Joe Herbertson,et al. Experimental Studies of Interfacial Heat Transfer and Initial Solidification Pertinent to Strip Casting , 1998 .
[23] P. Lin,et al. Coincidence Site Lattice (CSL) grain boundaries and Goss texture development in Fe-3% Si alloy , 1996 .
[24] T. Mizoguchi,et al. Formation of Solidification Structure in Twin Roll Casting Process of 18Cr-8Ni Stainless Steel , 1995 .
[25] Y. Ushigami,et al. Magnetic properties of (110)[001] grain oriented 6.5% silicon steel , 1991 .
[26] Munetsugu Matsuo,et al. Texture Control in the Production of Grain Oriented Silicon Steels , 1989 .
[27] H. Inagaki,et al. The Development of Rolling Textures in Low-Carbon Steels , 1972 .