Fire retardant action of mineral fillers

Endothermically decomposing mineral fillers, such as aluminium or magnesium hydroxide, magnesium carbonate, or mixed magnesium/calcium carbonates and hydroxides, such as naturally occurring mixtures of huntite and hydromagnesite are in heavy demand as sustainable, environmentally benign fire retardants. They are more difficult to deploy than the halogenated flame retardants they are replacing, as their modes of action are more complex, and are not equally effective in different polymers. In addition to their presence (at levels up to 70%), reducing the flammable content of the material, they have three quantifiable fire retardant effects: heat absorption through endothermic decomposition; increased heat capacity of the polymer residue; increased heat capacity of the gas phase through the presence of water or carbon dioxide. These three contributions have been quantified for eight of the most common fire retardant mineral fillers, and the effects on standard fire tests such as the LOI, UL 94 and cone calorimeter discussed. By quantifying these estimable contributions, more subtle effects, which they might otherwise mask, may be identified.

[1]  T. R. Hull,et al.  Decomposition and combustion of EVA and LDPE alone and when fire retarded with ATH , 2000 .

[2]  T. Hull,et al.  The fire retardant behaviour of huntite and hydromagnesite – A review , 2010 .

[3]  Serge Bourbigot,et al.  Mechanisms of Smoke and CO Suppression from EVA Composites , 2005 .

[4]  J. Milewski,et al.  Handbook Of Fillers For Plastics , 1987 .

[5]  B. Schartel,et al.  Temperature inside burning polymer specimens: Pyrolysis zone and shielding , 2009 .

[6]  T. R. Hull,et al.  An investigation into the decomposition and burning behaviour of ethylene-vinyl acetate copolymer nanocomposite materials , 2003 .

[7]  Richard E. Lyon,et al.  The effect of variation in polymer properties on the rate of burning , 2009 .

[8]  S. Shaw Halogenated Flame Retardants: Do the Fire Safety Benefits Justify the Risks? , 2010, Reviews on environmental health.

[9]  D. Ruch,et al.  A comparison of the role of boehmite (AlOOH) and alumina (Al2O3) in the thermal stability and flammability of poly(methyl methacrylate) , 2009 .

[10]  Barbara C. Levin,et al.  Toxicity of the pyrolysis and combustion products of poly(vinyl chlorides): A literature assessment , 1986 .

[11]  Yu-Zhong Wang,et al.  Effect of metal chelates on the ignition and early flaming behaviour of intumescent fire-retarded polyethylene systems , 2008 .

[12]  P. Hornsby,et al.  Flame retardant effects of magnesium hydroxide , 1996 .

[13]  C. D. de Wit An overview of brominated flame retardants in the environment. , 2002, Chemosphere.

[14]  Hydrogen Chloride in Fires , 2008 .

[15]  T. R. Hull,et al.  Flame retardance of poly(methyl methacrylate) modified with phosphorus-containing compounds , 2002 .

[16]  T. R. Hull,et al.  Fire Retardancy of Polymers: New Strategies and Mechanisms , 2008 .

[17]  P. S. Santos,et al.  Standard transition aluminas. Electron microscopy studies , 2000 .

[18]  J. Torero,et al.  Flammability assessment of tannin-based cellular materials , 2011 .

[19]  S. Bourbigot,et al.  Recent advances in the use of zinc borates in flame retardancy of EVA , 1999 .

[20]  T. R. Hull,et al.  Flame retardancy of some ethylene–vinyl acetate copolymer‐based formulations , 2000 .

[21]  A. Stec,et al.  Fire retardant effects of polymer nanocomposites. , 2009, Journal of nanoscience and nanotechnology.

[22]  Keith T. Paul Feasibility study to demonstrate the potential of smoke hoods in simulated aircraft fire atmospheres: Development of the fire model , 1989 .

[23]  T. R. Hull,et al.  Combustion toxicity of fire retarded EVA , 2002 .

[24]  T. R. Hull,et al.  Fire retardancy of a reactively extruded intumescent flame retardant polyethylene system enhanced by metal chelates , 2007 .

[25]  R. Rothon Particulate-filled Polymer Composites , 1995 .

[26]  Charles A. Wilkie,et al.  Fire retardancy of polymeric materials , 2000 .

[27]  Q. Ji,et al.  Thermal stability and flame-retardancy mechanism of poly(ethylene terephthalate)/boehmite nanocomposites , 2010 .

[28]  S. Bourbigot,et al.  Nanomorphology and reaction to fire of polyurethane and polyamide nanocomposites containing flame retardants , 2010 .

[29]  Bernhard Schartel,et al.  Development of fire‐retarded materials—Interpretation of cone calorimeter data , 2007 .

[30]  Zhenzhong Li,et al.  Flammability characterization and synergistic effects of expandable graphite with magnesium hydroxide in halogen-free flame-retardant EVA blends , 2003 .

[31]  T. R. Hull,et al.  The thermal decomposition of huntite and hydromagnesite—A review☆ , 2010 .

[32]  P. Hornsby,et al.  A study of the mechanism of flame retardance and smoke suppression in polymers filled with magnesium hydroxide , 1990 .

[33]  M. Rigolo,et al.  Basic magnesium carbonate flame retardants for polypropylene , 2004 .