Fatigue Failure Modes of the Grain Size Transition Zone in a Dual Microstructure Disk

Mechanical property requirements vary with location in nickel-based superalloy disks. In order to maximize the associated mechanical properties, heat treatment methods have been developed for producing tailored grain microstructures. In this study, fatigue failure modes of a grain size transition zone in a dual microstructure disk were evaluated. A specialized heat treatment method was applied to produce varying grain microstructure in the bore to rim portions of a powder metallurgy processed nickel-based superalloy disk. The transition in grain size was concentrated in a zone of the disk web, between the bore and rim. Specimens were extracted parallel and transversely across this transition zone, and multiple fatigue tests were performed at 427 C and 704 C. Grain size distributions were characterized in the specimens, and related to operative failure initiation modes. Mean fatigue life decreased with increasing maximum grain size, going out through the transition zone. The scatter in limited tests of replicates was comparable for failures of uniform gage specimens in all transition zone locations examined.

[1]  T. Gabb,et al.  Thermal and Mechanical Property Characterization of the Advanced Disk Alloy LSHR , 2013 .

[2]  D. Hornbach,et al.  DWELL NOTCH LOW CYCLE FATIGUE BEHAVIOR OF A POWDER METALLURGY NICKEL DISK ALLOY , 2012 .

[3]  C. Sudbrack,et al.  Fatigue Resistance of the Grain Size Transition Zone in a Dual Microstructure Superalloy Disk , 2011 .

[4]  Tresa M. Pollock,et al.  Crystallographic fatigue crack initiation in nickel-based superalloy René 88DT at elevated temperature , 2009 .

[5]  Mark Hardy,et al.  Environment and time dependent effects on the fatigue response of an advanced nickel based superalloy , 2009 .

[6]  T. Gabb,et al.  Effects of Temperature on Failure Modes for a Nickel-Base Disk Superalloy , 2007 .

[7]  Tiffany A. Biles,et al.  Effectiveness of Shot Peening In Suppressing Fatigue Cracking At Non-Metallic Inclusions In Udimet(Registered Trademark)720 , 2005 .

[8]  K. Perkins 'Process Development, Microstructure and Mechanical Property Evaluation of a Dual Microstructure Heat Treated Advanced Nickel Disc Alloy , 2008 .

[9]  A. Rosenberger,et al.  Evaluation of the Influence of Grain Structure on the Fatigue Variability of Waspaloy , 2008 .

[10]  T. Gabb,et al.  THE EFFECT OF DUAL MICROSTRUCTURE HEAT TREATMENT ON AN ADVANCED NICKEL-BASE DISK ALLOY , 2004 .

[11]  P. F. Browning,et al.  Effects of High Temperature Exposures on Fatigue Life of Disk Superalloys , 2004 .

[12]  S. Srivatsa,et al.  Control of Grain Size Via Forging Strain Rate Limits for R'88DT , 2000 .

[13]  R. Sprague,et al.  Superalloy Powder Processing, Properties, and Turbine Disk Applications , 1984 .

[14]  P. S. Mathur,et al.  Development of Hot Isostatically Pressed (As-HIP) Powder Metallurgy Rene' 95 Turbine Hardware , 1976 .

[15]  K. N. Smith A Stress-Strain Function for the Fatigue of Metals , 1970 .