Oxidation of orthopaedic UHMWPE.

Retrieved EtO sterilised acetabular cups usually show much less degradation than gamma-ray sterilised cups. Some of our retrieved EtO sterilised cups did, however, reveal unexpected bulk oxidation. It was observed that this oxidation was always accompanied by whitening of the material. This whitening was found to be due to a break-up of the compression moulded material into its original particles. It was noticed that there was no oxidation in all parts, where the break-up and whitening appeared. The oxidation did, however, occur exclusively in the parts where there was a badly consolidated material. Upon examining shelf aged, unsterilised samples, it was found that the degradation was also present here. This shows that the observed phenomenon is not due to the service in vivo and that it must originate from the processing step. Just as for the retrieved samples, the shelf aged cups only showed oxidation in the bulk and not at the surface. It was concluded that the material used for the cups had been badly fused together during the compression moulding and that the machining had created a bad stress situation in the cups leading to a break-up of the particles. The mechanism that initiates the oxidation is not known, but it is believed that the distribution depends on how the internal stresses have acted to break up the structure. In the areas where the particles have been separated, there is probably a higher availability of oxygen than what is normally observed in UHMWPE.

[1]  I. Blakey,et al.  Raman spectral mapping of photo-oxidised polypropylene , 2000 .

[2]  R Pietrabissa,et al.  Wear of polyethylene cups in total hip arthroplasty: a parametric mathematical model. , 1998, Medical engineering & physics.

[3]  D. Chenery Detection of peroxy species in ultra-high-molecular-weight polyethylene by Raman spectroscopy. , 1997, Biomaterials.

[4]  A. Edidin,et al.  Advances in the processing, sterilization, and crosslinking of ultra-high molecular weight polyethylene for total joint arthroplasty. , 1999, Biomaterials.

[5]  P. Gao,et al.  The structure and rheology of molten ultra-high-molecular-mass polyethylene , 1994 .

[6]  J. Pospíšil,et al.  Oxidation inhibition in organic materials , 1990 .

[7]  W H Harris,et al.  Gamma sterilization of UHMWPE articular implants: an analysis of the oxidation problem. Ultra High Molecular Weight Poly Ethylene. , 1996, Biomaterials.

[8]  D. Bassett,et al.  On morphology of consolidated UHMWPE resin in hip cups. , 1999, Biomaterials.

[9]  L. Costa,et al.  Oxidation in orthopaedic UHMWPE sterilized by gamma-radiation and ethylene oxide. , 1998, Biomaterials.

[10]  B. Yeom,et al.  Profile of oxidation in irradiated polyethylene , 1998 .

[11]  V. Brunella,et al.  Effects of microtomy on the material properties of Ultra High Molecular Weight Polyethylene , 2001 .

[12]  G. Camino,et al.  Unacceptable biodegradation of polyethylene in vivo. , 1996, Biomaterials.

[13]  L. Costa,et al.  Analysis of products diffused into UHMWPE prosthetic components in vivo. , 2001, Biomaterials.

[14]  L. Costa,et al.  In vivo UHMWPE biodegradation of retrieved prosthesis. , 1998, Biomaterials.

[15]  F. Shen,et al.  Hydroperoxide formation in irradiated polyethylene , 1999 .

[16]  F. Shen,et al.  Potential errors in FTIR measurement of oxidation in ultrahigh molecular weight polyethylene implants. , 1999, Journal of biomedical materials research.

[17]  D. Rueda,et al.  An i.r. study of the “amorphous” phase in melt crystallized polyethylene , 1978 .

[18]  T. Mittlmeier,et al.  Characterization of UHMWPE hip cups run on joint simulators. , 1987, Journal of biomedical materials research.

[19]  T. Reitberger,et al.  Fracture of some polymers as studied with stress chemiluminescence (SCL) , 2000 .

[20]  S. Shalaby,et al.  Properties of self-reinforced ultra-high-molecular-weight polyethylene composites. , 1997, Biomaterials.

[21]  D. Farrar,et al.  The microstructure of ultra-high molecular weight polyethylene used in total joint replacements. , 1997, Biomaterials.