Corrosion resistance and mechanism of CeN, TiN and CeN/TiN bilayer composite film deposited by dual ion beam sputtering

[1]  Zhijun Han,et al.  A comparative study of the corrosion performance of titanium (Ti), titanium nitride (TiN), titanium dioxide (TiO2) and nitrogen-doped titanium oxides (N–TiO2), as coatings for biomedical applications , 2015 .

[2]  Yan-ping Wu,et al.  Microstructure and corrosion resistance of Cr/Cr2N multilayer film deposited on the surface of depleted uranium , 2014 .

[3]  Xiaolin Wang,et al.  Recent advances in study of uranium surface chemistry in China , 2014 .

[4]  R. Mccabe,et al.  Filiform-mode hydride corrosion of uranium surfaces , 2013 .

[5]  A. Krella Cavitation erosion resistance of Ti/TiN multilayer coatings , 2013 .

[6]  Hui Yang,et al.  Study of behaviors of aluminum overlayers deposited on uranium via AES, EELS, and XPS , 2013 .

[7]  H. H. Caicedo,et al.  Nature in corrosion–erosion surface for [TiN/TiAlN]n nanometric multilayers growth on AISI 1045 steel , 2012 .

[8]  Y. Ping Physicochemical Properties of Simulated Radioactive Waste Formed with Cerium , 2012 .

[9]  Zha Yan-hong Crystal Lattice Immobilization of Perovskite for Simulation Uranium , 2012 .

[10]  C. V. Muraleedharan,et al.  A comparative study of titanium nitride (TiN), titanium oxy nitride (TiON) and titanium aluminum nitride (TiAlN), as surface coatings for bio implants , 2011 .

[11]  M. Odén,et al.  Machining performance and decomposition of TiAlN/TiN multilayer coated metal cutting inserts , 2011 .

[12]  J. Flis,et al.  Corrosion and passivation of iron and its nitrided layer in borate buffer , 2009 .

[13]  Z. Ping,et al.  Investigation of oxidation of a U‐2.5 wt% Nb alloy in air at low temperatures: kinetic study and oxide characterization , 2008 .

[14]  C. Dong,et al.  TiN, TiN gradient and Ti/TiN multi-layer protective coatings on Uranium , 2007 .

[15]  Da-yung Wang,et al.  Characterization of nanocrystalline AlTiN coatings synthesized by a cathodic-arc deposition process , 2007 .

[16]  H. Barshilia,et al.  Electrochemical behavior of single layer CrN, TiN, TiAlN coatings and nanolayered TiAlN/CrN multilayer coatings prepared by reactive direct current magnetron sputtering , 2006 .

[17]  A. Lavacchi,et al.  High-temperature oxidation of CrN/AlN multilayer coatings , 2005 .

[18]  L. Dobrzański,et al.  Structure and properties of selected cemented carbides and cermets covered with TiN/(Ti,Al,Si)N/TiN coatings obtained by the cathodic arc evaporation process , 2005 .

[19]  Ju-liang He,et al.  Corrosion and cell adhesion behavior of TiN-coated and ion-nitrided titanium for dental applications , 2005 .

[20]  R. Field,et al.  Microtextural investigation of hydrided α-uranium , 2004 .

[21]  M. Scheib,et al.  Cathodic arc evaporation of (Ti,Al)N coatings and (Ti,Al)N/TiN multilayer-coatings—correlation between lifetime of coated cutting tools, structural and mechanical film properties , 2004 .

[22]  S. Mikhailov,et al.  Depth profiles study of n(TiN+AlN) bilayers systems by GDOES and RBS techniques , 2003 .

[23]  Ying Li,et al.  The electrochemical corrosion behavior of TiN and (Ti,Al)N coatings in acid and salt solution , 2003 .

[24]  G. Kimmel,et al.  Long-term amorphisation of C+ and N2+ implanted layers on a uranium surface , 2002 .

[25]  Chen Nuo-fu,et al.  The pl “violet shift” of cerium dioxide on silicon , 2001 .

[26]  J. Baranowska,et al.  Cathode sputtering as a pre-treatment for gas nitriding , 2001 .

[27]  J. Gibson,et al.  Synthesis and Investigation of Plutonium Oxide Cluster Ions:PuxOy+(x(<)(=)18) , 2001 .

[28]  J. Albella,et al.  Low grain size TiN thin films obtained by low energy ion beam assisted deposition , 2001 .

[29]  M. Mintz,et al.  Passivation of uranium towards air corrosion by N2+ and C+ ion implantation , 2000 .

[30]  Thierry Czerwiec,et al.  Low-pressure, high-density plasma nitriding: mechanisms, technology and results , 1998 .

[31]  C. V. Cooper,et al.  Observation of a compound layer with very low friction coefficient in ion-nitrided martensitic 410 stainless steel , 1998 .

[32]  C. V. Cooper,et al.  Conditions for the formation of a martensitic single-phase compound layer in ion-nitrided 316L austenitic stainless steel , 1998 .

[33]  J. Bloch,et al.  Kinetics and mechanisms of metal hydrides formation—a review , 1997 .

[34]  R. Greenwood,et al.  Studies of the kinetics and mechanism of the oxidation of uranium by dry and moist air A model for determining the oxidation rate over a wide range of temperatures and water vapour pressures , 1994 .

[35]  W. Ensinger,et al.  Are coatings produced by ion-beam-assisted deposition superior? A comparison of chemical and mechanical properties of steel coated using different deposition techniques , 1992 .

[36]  M. J. Kane,et al.  Adhesion and corrosion behavior of Al-Zn and TiN/Ti/TiN coatings on a DU-0.75wt.% Ti alloy , 1991 .

[37]  W. Nowak,et al.  Assessment of corrosion-resistant coatings for a depleted uranium-0.75 titanium alloy , 1991 .

[38]  G. C. Allen,et al.  The behaviour of uranium metal in hydrogen atmospheres , 1988 .

[39]  S. Randles,et al.  The kinetics of the uranium-oxygen-water vapour reaction between 40 and 100°c , 1986 .

[40]  C. Colmenares Oxidation mechanisms and catalytic properties of the actinides , 1985 .

[41]  A. G. Ritchie,et al.  A review of the rates of reaction of uranium with oxygen and water vapour at temperatures up to 300° c , 1981 .