Microstructure and mechanical properties of the α-SiAlON/α-SiC composites: Effects of heat treatment
暂无分享,去创建一个
Yu Zhou | F. Ye | Limeng Liu
[1] D. Basu,et al. Influence of SiC addition on tribological properties of SiAlON , 2011 .
[2] D. Kim,et al. Enhanced sintering of SiC using infiltration of preceramic polymer , 2011 .
[3] D. Turan,et al. High temperature bending creep behavior of a multi-cation doped α/β-SiAlON composite , 2011 .
[4] Yu Zhou,et al. Elongation of α‐SiC Particles in Spark Plasma Sintered α‐SiAlON/α‐SiC Composites , 2011 .
[5] D. Bučevac,et al. Toughening of SiC matrix with in-situ created TiB2 particles , 2010 .
[6] O. Silva,et al. α-SiAlON–SiC composites obtained by gas-pressure sintering and hot-pressing , 2007 .
[7] O. Silva,et al. Development of α-SiAlON-SiC ceramic composites by liquid phase sintering , 2007 .
[8] M. Nygren,et al. Homogeneity Region and Thermal Stability of Neodymium‐Doped α‐Sialon Ceramics , 2005 .
[9] I. Chen,et al. Effect of Seeding on the Microstructure and Mechanical Properties of α‐SiAlON: I, Y‐SiAlON , 2004 .
[10] M. Nygren,et al. Formation of in situ reinforced microstructures in α-sialon ceramics: Part III. Static and dynamic ripening , 2004 .
[11] Michael J. Hoffmann,et al. Effect of the Amount of Additives and Post-Heat Treatment on the Microstructure and Mechanical Properties of Yttrium–α-Sialon Ceramics , 2003 .
[12] Joosung Kim,et al. Effects of isothermal annealing on the microstructure and mechanical properties of SiC ceramics hot-pressed with Y2O3 and Al2O3 additions , 2002 .
[13] M. Herrmann,et al. The effect of processing conditions, amount of additives and composition on the microstructures and mechanical properties of α-SiAlON ceramics , 2002 .
[14] K. Komeya,et al. Inhomogeneous grain growth and elongation of Dy-α sialon ceramics at temperatures above 1800°C , 2000 .
[15] Young‐Wook Kim,et al. Strength and fracture toughness of in situ-toughened silicon carbide , 1997 .
[16] T. Ekstrom,et al. Simultaneously MoSi2 and SiC-reinforced α-SiAlON composites , 1997 .
[17] Hong Wang,et al. Microstructure and mechanical properties of nanoscale SiC/Ca α-SiAlON composites , 1997 .
[18] S. Dong,et al. Hot isostatic pressing and post-hot isostatic pressing of SiC-β-sialon composites , 1996 .
[19] Chun-Hway Hsueh,et al. Debonding of interfaces between beta-silicon nitride whiskers and SiAlY oxynitride glasses , 1996 .
[20] L. C. Jonghe,et al. In Situ Toughened Silicon Carbide with Al‐B‐C Additions , 1996 .
[21] S. K. Lee. Effects of [alpha]-SiC versus [beta]-SiC starting powders on microstructure and fracture toughness of SiC sintered with Al[sub 2]O[sub 3]-Y[sub 2]O[sub 3] additives , 1994 .
[22] P. Becher. Microstructural design of toughened ceramics , 1991 .
[23] D. Clarke. On the Equilibrium Thickness of Intergranular Glass Phases in Ceramic Materials , 1987 .
[24] G. A. Slack,et al. Solubility of Carbon in Silicon and Germanium , 1959 .