Thermally induced changes in dynamic mechanical properties of native silks.

Dynamic mechanical thermal analysis (DMTA) on individual native silk fibers demonstrates changes in the dynamic mechanical properties of storage modulus and loss tangent as a function of temperature and temperature history ranging from -100 to 250 °C. These property changes are linked quantitatively to two main types of change in the silk structure. First, the evaporation of water with increasing temperature up to 100 °C increases the storage modulus and removes two characteristic loss tangent peaks at -60 and +60 °C. Second, various discrete loss tangent peaks in the range 150-220 °C are associated with specific disordered silk structures that are removed or converted to a limiting high-temperature relaxed structure by the combination of increasing temperature and static load in the DMTA tests. The results identify important origins of silk filament quality based on the analysis of measurements that can be traced back to differences in production and processing history.

[1]  Todd A Blackledge,et al.  Quasistatic and continuous dynamic characterization of the mechanical properties of silk from the cobweb of the black widow spider Latrodectus hesperus , 2005, Journal of Experimental Biology.

[2]  D. Porter,et al.  The role of kinetics of and amide bonding in protein stability. , 2008, Soft matter.

[3]  D. Porter,et al.  Predictive nonlinear constitutive relations in polymers through loss history , 2009 .

[4]  D. Porter,et al.  Proline and processing of spider silks. , 2008, Biomacromolecules.

[5]  D. Porter,et al.  Water mobility, denaturation and the glass transition in proteins. , 2012, Biochimica et biophysica acta.

[6]  D. Kaplan,et al.  Microphase Separation Controlled β-Sheet Crystallization Kinetics in Fibrous Proteins , 2009 .

[7]  Shigeo Nakamura,et al.  Thermal Properties of Silk Proteins in Silkworms , 1993 .

[8]  Z. Shao,et al.  Understanding the Mechanical Properties of Antheraea Pernyi Silk—From Primary Structure to Condensed Structure of the Protein , 2011 .

[9]  W. Doster The dynamical transition of proteins, concepts and misconceptions , 2008, European Biophysics Journal.

[10]  David L. Kaplan,et al.  Mechanical and thermal properties of dragline silk from the spider Nephila clavipes , 1994 .

[11]  Blas Echebarria,et al.  Supernormal conduction in cardiac tissue promotes concordant alternans and action potential bunching. , 2011, Physical review. E, Statistical, nonlinear, and soft matter physics.

[12]  D. Porter,et al.  Spider silk as a model biomaterial , 2006 .

[13]  P. Zhou,et al.  Toughness of Spider Silk at High and Low Temperatures , 2005 .

[14]  David L. Kaplan,et al.  Effect of water on the thermal properties of silk fibroin , 2007 .

[15]  David L. Kaplan,et al.  Dynamic Protein−Water Relationships during β-Sheet Formation , 2008 .

[16]  D. Porter,et al.  Silks cope with stress by tuning their mechanical properties under load , 2012 .

[17]  Z. Shao,et al.  Moisture Effects on Antheraea pernyi Silk's Mechanical Property , 2009 .

[18]  T. Seydel,et al.  Increased molecular mobility in humid silk fibers under tensile stress. , 2011, Physical review. E, Statistical, nonlinear, and soft matter physics.

[19]  David L. Kaplan,et al.  Determining Beta-Sheet Crystallinity in Fibrous Proteins by Thermal Analysis and Infrared Spectroscopy , 2006 .

[20]  Fritz Vollrath,et al.  Materials: Surprising strength of silkworm silk , 2002, Nature.

[21]  Ingi Agnarsson,et al.  How super is supercontraction? Persistent versus cyclic responses to humidity in spider dragline silk , 2009, Journal of Experimental Biology.

[22]  Jinrong Yao,et al.  Kinetics of thermally-induced conformational transitions in soybean protein films , 2010 .

[23]  G. Plaza,et al.  Thermo‐hygro‐mechanical behavior of spider dragline silk: Glassy and rubbery states , 2006 .

[24]  Jinrong Yao,et al.  Correlation between structural and dynamic mechanical transitions of regenerated silk fibroin , 2010 .

[25]  F Vollrath,et al.  Predicting the mechanical properties of spider silk as a model nanostructured polymer , 2005, The European physical journal. E, Soft matter.

[26]  C. Migliaresi,et al.  Regenerated silk fibroin films: Thermal and dynamic mechanical analysis , 2002 .

[27]  D. Porter,et al.  Two mechanisms for supercontraction in Nephila spider dragline silk. , 2011, Biomacromolecules.

[28]  Z. Shao,et al.  A kinetic model for thermal degradation in polymers with specific application to proteins , 2009 .