Thermal degradation of wood treated with creosote
暂无分享,去创建一个
[1] Antonius Kettrup,et al. Thermal analysis-mass spectrometry and thermogravimetric adsorption on fire retardants , 1990 .
[2] R. Marutzky. Disposal of wood treated with preservatives: possibilities and problems. , 1990 .
[3] A. Kettrup,et al. Thermal degradation of polymers and flame retardants , 1989 .
[4] A. Kettrup,et al. The pyrolysis of polymers and identification of the soot adsorbed components , 1989 .
[5] A. Kettrup,et al. TA-MS investigations of coal westerholt and its related asphaltene and asphal-tole , 1987 .
[6] A. Kettrup,et al. Computer - aided simultaneous TA-MS investigations of beat-resistant polystyrene , 1987 .
[7] K. Ohrbach,et al. Application of combined thermal analysis - mass spectrometry in the analysis of fossil fuels and polymers , 1985 .
[8] Antonius Kettrup,et al. Investigations of the thermal decomposition of PVC cable material by means of simultaneous TG-DTG-DTA-MS analysis , 1985 .
[9] A. Kettrup,et al. The thermal degradation of a polyurethane foam containing the flame-retardant tetrakis(2-chloroethyl) ethylenediphosphate using simultaneous thermal analysis-mass spectrometry , 1985 .
[10] F. A. Patty,et al. Patty's Industrial hygiene and toxicology , 1978 .