Comparative Investigation of Tungsten Fibre Nets Reinforced Tungsten Composite Fabricated by Three Different Methods

Tungsten fibre nets reinforced tungsten composites (Wf/W) containing four net layers were fabricated by spark plasma sintering (SPS), hot pressing (HP) and cold rolling after HP (HPCR), with the weight fraction of fibres being 17.4%, 10.5% and 10.5%, respectively. The relative density of the HPCRed samples is the highest (99.8%) while that of the HPed composites is the lowest (95.1%). Optical and scanning electron microscopy and electron back scattering diffraction were exploited to characterize the microstructure, while tensile and hardness tests were used to evaluate the mechanical properties of the samples. It was found that partial recrystallization of fibres occurred after the sintering at 1800 °C. The SPSed and HPed Wf/W composites begin to exhibit plastic deformation at 600 °C with tensile strength (TS) of 536 and 425 MPa and total elongation at break (TE) of 11.6% and 23.0%, respectively, while the HPCRed Wf/W composites exhibit plastic deformation at around 400 °C. The TS and TE of the HPCRed Wf/W composites at 400 °C are 784 MPa and 8.4%, respectively. The enhanced mechanical performance of the Wf/W composites over the pure tungsten can be attributed to the necking, cracking, and debonding of the tungsten fibres.

[1]  C. S. Liu,et al.  Toughness enhancement of tungsten reinforced with short tungsten fibres , 2017 .

[2]  G. Lu,et al.  A comparison of interatomic potentials for modeling tungsten nanocluster structures , 2017 .

[3]  C. Parish,et al.  Effect of starting microstructure on helium plasma-materials interaction in tungsten , 2017 .

[4]  Gerald Pintsuk,et al.  Advanced materials for a damage resilient divertor concept for DEMO: Powder-metallurgical tungsten-fibre reinforced tungsten , 2017 .

[5]  R. Neu,et al.  Chemically deposited tungsten fibre-reinforced tungsten – The way to a mock-up for divertor applications , 2016 .

[6]  B. Wirth,et al.  Irradiation hardening of pure tungsten exposed to neutron irradiation , 2016 .

[7]  R. Elliman,et al.  Effect of rhenium irradiations on the mechanical properties of tungsten for nuclear fusion applications , 2016 .

[8]  I. Uytdenhouwen,et al.  Investigation of the combined effect of neutron irradiation and electron beam exposure on pure tungsten , 2016 .

[9]  Xianping Wang,et al.  High strength and thermal stability of bulk Cu/Ta nanolamellar multilayers fabricated by cross accumulative roll bonding , 2016 .

[10]  Zhengyuan Gao,et al.  Enhancing Thermal Conductivity of Mg-Sn Alloy Sheet by Cold Rolling and Aging , 2016, Journal of Materials Engineering and Performance.

[11]  C. S. Liu,et al.  Toughness and microstructure of tungsten fibre net-reinforced tungsten composite produced by spark plasma sintering , 2016 .

[12]  X. P. Wang,et al.  Effect of hot rolling and annealing on the mechanical properties and thermal conductivity of W-0.5wt.% TaC alloys , 2016 .

[13]  R. Liu,et al.  High thermal shock resistance of the hot rolled and swaged bulk W–ZrC alloys , 2016 .

[14]  M. Rieth,et al.  Ductilisation of tungsten (W): On the shift of the brittle-to-ductile transition (BDT) to lower temperatures through cold rolling , 2016 .

[15]  C. S. Liu,et al.  Grain growth behavior and mechanical properties of zirconium micro-alloyed and nano-size zirconium carbide dispersion strengthened tungsten alloys , 2015 .

[16]  M. Bram,et al.  Powder Metallurgical Tungsten Fiber-Reinforced Tungsten , 2015 .

[17]  Leena‐Sisko Johansson,et al.  Hydrofluoric-nitric-sulphuric-acid surface treatment of tungsten for carbon fibre-reinforced composite hybrids in space applications , 2015 .

[18]  C. S. Liu,et al.  Fabricating high performance tungsten alloys through zirconium micro-alloying and nano-sized yttria dispersion strengthening , 2014 .

[19]  J.-H. You,et al.  Enhanced toughness and stable crack propagation in a novel tungsten fibre-reinforced tungsten composite produced by chemical vapour infiltration , 2014 .

[20]  X. P. Wang,et al.  Spark plasma sintering and mechanical properties of zirconium micro-alloyed tungsten , 2014 .

[21]  K. Cui,et al.  Microstructural characteristics of commercial purity W and W–1% La2O3 alloy , 2013 .

[22]  J.-H. You,et al.  In situ synchrotron tomography estimation of toughening effect by semi-ductile fibre reinforcement in a tungsten-fibre-reinforced tungsten composite system , 2013 .

[23]  Song Zhang,et al.  Fabrication and properties of W–20Cu alloy reinforced by titanium nitride coated SiC fibers , 2013 .

[24]  C. Dong,et al.  Anisotropic compressive deformation behaviors of tungsten fiber reinforced Zr-based metallic glass composites , 2013 .

[25]  L. Qian Recrystallization and texture of tungsten strip , 2013 .

[26]  T. Höschen,et al.  Shear debonding behavior of a carbon-coated interface in a tungsten fiber-reinforced tungsten matrix composite , 2011 .

[27]  T. Höschen,et al.  Feasibility Study of a Tungsten Wire Reinforced Tungsten Matrix Composite with ZrOx Interfacial Coatings , 2010 .

[28]  T. Höschen,et al.  Interfacial fracture behavior of tungsten wire/tungsten matrix composites with copper-coated interfaces , 2010 .

[29]  N. Shi,et al.  Microstructure Characterization of Long W Core SiC Fiber , 2007 .

[30]  Z. Meiling,et al.  The recrystallization mechanism of doped tungsten wire , 1990 .