Stone Endurance: A Comparative Analysis of Natural and Artificial Weathering on Stone Longevity
暂无分享,去创建一个
J. Mirão | F. Sitzia | Carla Lisci | V. Pires | Mauro Francesco | La Russa | Patricia Sanmart í n | Marco Aniceto | Jos é Mir ã o | C. Lisci
[1] J. Mirão,et al. Laboratorial Simulation for Assessing the Performance of Slates as Construction Materials in Cold Climates , 2023, Applied Sciences.
[2] J. Mirão,et al. The interaction between rainwater and polished building stones for flooring and cladding - Implications in architecture , 2022, Journal of Building Engineering.
[3] P. M. Amaral,et al. Experimental procedure for studying the degradation and alteration of limestone slabs applied on exterior cladding , 2021, Environmental Earth Sciences.
[4] P. Peikertová,et al. Long-term effect of weather in Dfb climate subtype on properties of hydrophobic coatings on sandstone , 2022, Journal of Building Engineering.
[5] S. Siegesmund,et al. Petrophysical Properties of Limestones - Influence On Behaviour Under Different Environmental Conditions And Applications , 2021 .
[6] J. Mirão,et al. Building pathology and environment: Weathering and decay of stone construction materials subjected to a Csa mediterranean climate laboratory simulation , 2021 .
[7] M. Frigione,et al. Novel Nano-Filled Coatings for the Protection of Built Heritage Stone Surfaces , 2021, Nanomaterials.
[8] J. Mirão,et al. Accelerate ageing on building stone materials by simulating daily, seasonal thermo-hygrometric conditions and solar radiation of Csa Mediterranean climate , 2021 .
[9] F. Sitzia,et al. Pyroclastic Stones as Building Materials in Medieval Romanesque Architecture of Sardinia (Italy): Chemical-Physical Features of Rocks and Associated Alterations , 2020, International Journal of Architectural Heritage.
[10] I. Flores-Colen,et al. Effect of Hygrothermal Aging on Hydrophobic Treatments Applied to Building Exterior Claddings , 2020, Coatings.
[11] J. Orlowsky,et al. The Influence of 30 Years Outdoor Weathering on the Durability of Hydrophobic Agents Applied on Obernkirchener Sandstones , 2020, Buildings.
[12] Sumit Parvate,et al. Superhydrophobic Surfaces: Insights from Theory and Experiment. , 2020, The journal of physical chemistry. B.
[13] P. Moita,et al. Natural limestone discolouration triggered by microbial activity—a contribution , 2018, AIMS microbiology.
[14] M. S. Akram,et al. Prediction of mechanical behaviour from mineralogical composition of Sakesar limestone, Central Salt Range, Pakistan , 2017, Bulletin of Engineering Geology and the Environment.
[15] M. Frigione,et al. Durability of a sunlight-curable organic–inorganic hybrid protective coating for porous stones in natural and artificial weathering conditions , 2016 .
[16] P. Marini,et al. Ten years of natural ageing of calcareous stones , 2016 .
[17] A. Sansonetti,et al. Evaluation of Moisture Transfer to Improve the Conservation of Tiles Finishing Facades , 2016 .
[18] J. Neshati,et al. Improving the UV degradation resistance of epoxy coatings using modified carbon black nanoparticles , 2015 .
[19] A. Balbo,et al. Organosilane coatings applied on bronze: Influence of UV radiation and thermal cycles on the protectiveness , 2015 .
[20] A. M. Mecchi,et al. The role of the petrophysical characteristics on the durability and conservation of some porous calcarenites from Southern Italy , 2015, Special Publications.
[21] G. R. Khanlari,et al. Influence of wet–dry, freeze–thaw, and heat–cool cycles on the physical and mechanical properties of Upper Red sandstones in central Iran , 2015, Bulletin of Engineering Geology and the Environment.
[22] M. Urošević,et al. An experimental study on the influence of surface finishing on the weathering of a building low-porous limestone in coastal environments , 2013 .
[23] A. Khanna,et al. Anticorrosion performance of eco-friendly silane primer for coil coating applications , 2012 .
[24] Bjørn Petter Jelle,et al. Accelerated climate ageing of building materials, components and structures in the laboratory , 2012, Journal of Materials Science.
[25] P. Gane,et al. Robust hydrophobic surfaces displaying different surface roughness scales while maintaining the same wettability. , 2011, Langmuir : the ACS journal of surfaces and colloids.
[26] Katarina Malaga,et al. Definition of the procedure to determine the suitability and durability of an anti-graffiti product for application on cultural heritage porous materials , 2011 .
[27] Joann M. Taylor,et al. Digital Color Imaging Handbook , 2004 .
[28] Francisco M. Martínez-Verdú,et al. Influence of Surface Roughness on Color Changes in Building Stones , 2003 .
[29] Maria João Melo,et al. Correlating natural ageing and Xenon irradiation of Paraloid® B72 applied on stone , 2003 .
[30] C.Y. Jim,et al. Alkaline rains on the Tibetan Plateau and their implication for the original pH of natural rainfall , 2002 .
[31] N. Middleton,et al. Saharan dust storms: nature and consequences , 2001 .
[32] Atiye Tugrul,et al. Engineering aspects of limestone weathering in Istanbul, Turkey , 2000 .
[33] F. Millero,et al. A CHEMICAL EQUILIBRIUM MODEL FOR THE CARBONATE SYSTEM IN NATURAL WATERS , 1997 .
[34] Rob B. Polder,et al. Hydrophobic treatment of concrete , 1997 .
[35] A. Cassie,et al. Wettability of porous surfaces , 1944 .
[36] R. N. Wenzel. RESISTANCE OF SOLID SURFACES TO WETTING BY WATER , 1936 .
[37] Thomas Young,et al. An Essay on the Cohesion of Fluids , 1800 .