Hydrogen embrittlement behavior in the nugget zone of friction stir welded X100 pipeline steel

[1]  L.Y. Mao,et al.  Hydrogen embrittlement behavior in interstitial Mn–N austenitic stainless steel , 2022, International Journal of Hydrogen Energy.

[2]  G.D. Wang,et al.  Achievement of excellent strength and plasticity in the nugget zone of friction stir welded bainitic steel and its deformation behavior , 2022, Journal of Materials Research and Technology.

[3]  Xiao-nan Wang,et al.  Effect of microstructure homogeneity on the impact fracture mechanism of X100 pipeline steel laser–MAG hybrid welds with an alternating magnetic field , 2022, Materials Science and Engineering: A.

[4]  Ying Sun,et al.  Hydrogen-induced degradation of high-strength steel pipeline welds: A critical review , 2022, Engineering Failure Analysis.

[5]  Lei Zhang,et al.  Effects of hydrogen on the fracture toughness of X80 steel base metal and girth weld under strong cathodic current with in-situ hydrogen charging , 2022, Engineering Failure Analysis.

[6]  K. Wu,et al.  Grain refinement strengthening mechanism of an austenitic stainless steel: critically analyze the impacts of grain interior and grain boundary , 2022, Journal of Materials Research and Technology.

[7]  Xiaodong Zhu,et al.  Effect of martensite morphology and volume fraction on the low-temperature impact toughness of dual-phase steels , 2021, Materials Science and Engineering: A.

[8]  L. Du,et al.  Investigation of austenite decomposition behavior and relationship to mechanical properties in continuously cooled medium-Mn steel , 2021, Materials Science and Engineering: A.

[9]  G.D. Wang,et al.  Crystallography of the nugget zone of bainitic steel by friction stir welding in various cooling mediums , 2021, Materials Characterization.

[10]  Shuang-jiang Li,et al.  Temperature Dependence of Deformation Behaviors in High Manganese Austenitic Steel for Cryogenic Applications , 2021, Materials.

[11]  W. B. Bose Filho,et al.  Hydrogen-induced cracking and corrosion behavior of friction stir welded plates of API 5L X70 pipeline steel , 2021, International Journal of Hydrogen Energy.

[12]  Y. F. Cheng,et al.  Hydrogen permeation and distribution at a high-strength X80 steel weld under stressing conditions and the implication on pipeline failure , 2021 .

[13]  R. Misra,et al.  Microstructural refinement mechanism and its effect on toughness in the nugget zone of high-strength pipeline steel by friction stir welding , 2021 .

[14]  L. Du,et al.  Hydrogen diffusivity in different microstructural components in martensite matrix with retained austenite , 2021 .

[15]  X. Xing,et al.  Quantification of the temperature threshold of hydrogen embrittlement in X90 pipeline steel , 2021 .

[16]  T. Nguyen,et al.  Hydrogen environment assisted cracking in X70 welding heat-affected zone under a high-pressure hydrogen gas , 2020 .

[17]  Yan-wen Tian,et al.  Effect of rolling reduction below γ non-recrystallization temperature on pancaked γ, microstructure, texture and low-temperature toughness for hot rolled steel , 2020 .

[18]  Wei Yan,et al.  Tensile deformation damage behavior of a high deformability pipeline steel with a ferrite and bainite microstructure , 2020 .

[19]  X. Di,et al.  The mutual effect of hydrogen and cyclic plastic deformation on ductility degradation of X65 reeled-pipeline welded joint , 2020 .

[20]  R. Misra,et al.  Microstructure, crystallography, and toughness in nugget zone of friction stir welded high-strength pipeline steel , 2020 .

[21]  E. Akiyama,et al.  Review of Hydrogen Embrittlement in Metals: Hydrogen Diffusion, Hydrogen Characterization, Hydrogen Embrittlement Mechanism and Prevention , 2020, Acta Metallurgica Sinica (English Letters).

[22]  Manish K Vishwakarma,et al.  Effect of hydrogen in advanced high strength steel materials , 2019, International Journal of Hydrogen Energy.

[23]  R.Z. Wang,et al.  Hydrogen embrittlement sensitivity of X100 pipeline steel under different pre-strain , 2019, International Journal of Hydrogen Energy.

[24]  A. P. Tschiptschin,et al.  Influence of hydrogen on the microstructure and fracture toughness of friction stir welded plates of API 5L X80 pipeline steel , 2019, International Journal of Hydrogen Energy.

[25]  Z. Ma,et al.  Microstructure and Mechanical Properties of X80 Pipeline Steel Joints by Friction Stir Welding Under Various Cooling Conditions , 2019, Acta Metallurgica Sinica (English Letters).

[26]  Seung-Yong Lee,et al.  Tensile and Fracture Behaviors of Austenitic High-Manganese Steels Subject to Different Hydrogen Embrittlement Test Methods , 2019, Materials Science and Engineering: A.

[27]  R. Kaibyshev,et al.  Microstructure evolution and strengthening mechanisms in friction-stir welded TWIP steel , 2019, Materials Science and Engineering: A.

[28]  Sandeep Kumar Dwivedi,et al.  Hydrogen embrittlement in different materials: A review , 2018, International Journal of Hydrogen Energy.

[29]  Sheng-wu Guo,et al.  Ultrafine grained dual-phase martensite/ferrite steel strengthened and toughened by lamella structure , 2018, Materials Science and Engineering: A.

[30]  Mingxing Zhang,et al.  Equivalent hydrogen fugacity during electrochemical charging of some martensitic advanced high-strength steels , 2017 .

[31]  M. Koyama,et al.  Overview of hydrogen embrittlement in high-Mn steels , 2017 .

[32]  Zhili Feng,et al.  Hydrogen accelerated fatigue crack growth of friction stir welded X52 steel pipe , 2017 .

[33]  L. Du,et al.  Hydrogen permeation behavior in relation to microstructural evolution of low carbon bainitic steel weldments , 2016 .

[34]  Yong Wang,et al.  Hydrogen permeation and embrittlement susceptibility of X80 welded joint under high-pressure coal gas environment , 2016 .

[35]  Mohammad Masoumi,et al.  Effect of crystallographic orientations on the hydrogen-induced cracking resistance improvement of API 5L X70 pipeline steel under various thermomechanical processing , 2016 .

[36]  T. Mcnelley,et al.  Effect of friction stir welding on hydrogen content of ISO 3183 X80M steel , 2016 .

[37]  H. Imai,et al.  Suppression of hydrogen-induced damage in friction stir welded low carbon steel joints , 2015 .

[38]  L. Du,et al.  Effect of microstructural constituents on strength–toughness combination in a low carbon bainitic steel , 2014 .

[39]  P. Xue,et al.  Enhanced mechanical properties in friction stir welded low alloy steel joints via structure refining , 2014 .

[40]  M. A. Mohtadi-Bonab,et al.  Evaluation of hydrogen induced cracking behavior of API X70 pipeline steel at different heat treatments , 2014 .

[41]  Yun-Hee Lee,et al.  Hydrogen-induced toughness drop in weld coarse-grained heat-affected zones of linepipe steel , 2013 .

[42]  K. Verbeken,et al.  Thermal desorption spectroscopy study of the interaction between hydrogen and different microstructural constituents in lab cast Fe–C alloys , 2012 .

[43]  M. Koyama,et al.  Effect of hydrogen content on the embrittlement in a Fe–Mn–C twinning-induced plasticity steel , 2012 .

[44]  H. Jing,et al.  Welding heat input effect on the hydrogen permeation in the X80 steel welded joints , 2012 .

[45]  Nack J. Kim,et al.  Effects of acicular ferrite on charpy impact properties in heat affected zones of oxide-containing API X80 linepipe steels , 2011 .

[46]  Y. F. Cheng,et al.  Effect of non-metallic inclusions on hydrogen-induced cracking of API5L X100 steel , 2010 .

[47]  O. Bouaziz,et al.  Effect of grain and twin boundaries on the hardening mechanisms of twinning-induced plasticity steels , 2008 .

[48]  Rajiv S. Mishra,et al.  Friction Stir Welding and Processing , 2007 .

[49]  E. A. Charles,et al.  Hydrogen embrittlement of high strength pipeline steels , 2006 .

[50]  W. Hutchinson,et al.  Transformation Textures in Steels , 2005 .

[51]  T. DebRoy,et al.  Absorption and transport of hydrogen during gas metal arc welding of low alloy steel , 1997 .

[52]  Mingxin Huang,et al.  Revisit the role of deformation twins on the work-hardening behaviour of twinning-induced plasticity steels , 2018 .

[53]  Y. Komizo,et al.  Microstructure and mechanical properties of friction stir welded X80 pipeline steel joint under additional cooling , 2013 .

[54]  Dierk Raabe,et al.  Deformation and fracture mechanisms in fine- and ultrafine-grained ferrite/martensite dual-phase steels and the effect of aging , 2011 .

[55]  H. Suzuki,et al.  Hydrogen assisted cracking in C-Mn and low alloy steel weldments , 1990 .