Autoclave tests of 64 K and 256 K SRAMs
暂无分享,去创建一个
Results are presented of HAST tests of 64 K and 256 K SRAMs of 10 manufacturers at three temperature/humidity conditions. Failed memory cells are clustered in four different, manufacturer dependent, ways. A relation between the type of defect cluster and weaknesses in the manufacturing process is presented.
[1] K. Fokkens,et al. Comparing HAST results of differently pretreated plastic encapsulated integrated circuits , 1989 .
[2] D. Danielson,et al. HAST applications: acceleration factors and results for VLSI components , 1989 .
[3] Christer Olsson. Reliability of plastic-encapsulated logic circuits , 1989 .
[4] T. Steiner,et al. Investigations of Large PLCC Package Cracking During Surface Mount Exposure , 1987 .