Reactive infiltration processing (RIP) of ultra high temperature ceramics (UHTC) into porous C/C composite tubes

[1]  Jenn‐Ming Yang,et al.  Microstructural development of a Cf/ZrC composite manufactured by reactive melt infiltration , 2010 .

[2]  A. Bellosi,et al.  Processing and properties of ultra-high temperature ceramics for space applications , 2008 .

[3]  Erica L. Corral,et al.  Ultra‐High‐Temperature Ceramic Coatings for Oxidation Protection of Carbon–Carbon Composites , 2008 .

[4]  杨嘉陵,et al.  Research Progress On Thermal Protection Materials And Structures Of Hypersonic Vehicles , 2008 .

[5]  E. Opila,et al.  UHTCs: Ultra-High Temperature Ceramic Materials for Extreme Environment Applications , 2007 .

[6]  Y. Yan,et al.  New Route to Synthesize Ultra‐Fine Zirconium Diboride Powders Using Inorganic–Organic Hybrid Precursors , 2006 .

[7]  A. Bellosi,et al.  The resistance to oxidation of an HfB2–SiC composite , 2005 .

[8]  Xiaohong Shi,et al.  Silicon carbide coating to protect carbon/carbon composites against oxidation , 2005 .

[9]  Raffaele Savino,et al.  Aerothermodynamic study of UHTC-based thermal protection systems , 2005 .

[10]  Donald T. Ellerby,et al.  High‐Strength Zirconium Diboride‐Based Ceramics , 2004 .

[11]  Donald T. Ellerby,et al.  Characterization of Zirconium Diboride for Thermal Protection Systems , 2004 .

[12]  Ruiying Luo,et al.  Thermophysical properties of carbon/carbon composites and physical mechanism of thermal expansion and thermal conductivity , 2004 .

[13]  Soojin Park,et al.  Studies on the mechanical and mechanical interfacial properties of carbon–carbon composites impregnated with an oxidation inhibitor , 2003 .

[14]  R. Menéndez,et al.  Influence of fibre–matrix interface on the fracture behaviour of carbon-carbon composites , 2003 .

[15]  A. Bellosi,et al.  Zirconium Diboride-Based Composites , 2001 .

[16]  R. Luo,et al.  Effect of additives on mechanical properties of oxidation-resistant carbon/carbon composite fabricated by rapid CVD method , 2000 .

[17]  R. E. Moore,et al.  Evolution of in Situ Refractories in the 20th Century , 1998 .

[18]  M. Inagaki,et al.  Improvement in properties and air oxidation resistance of carbon materials by boron oxide impregnation , 1997 .

[19]  Shanyi Du,et al.  Oxidation and ablation of 3D carbon-carbon composite at up to 3000 °C , 1995 .

[20]  Carlo G. Pantano,et al.  Synthesis and characterization of boron-doped carbons , 1995 .

[21]  Dan D. Edie,et al.  Carbon-Carbon Materials and Composites , 1994 .

[22]  J. Sheehan Chapter 8 – High-Temperature Coatings on Carbon Fibers and Carbon-Carbon Composites , 1993 .

[23]  P. George,et al.  ZrPt3 as a high-temperature, reflective, oxidation-resistant coating for carbon-carbon composites , 1991 .

[24]  S. Awasthi,et al.  C/C Composite Materials for Aircraft Brakes , 1988 .

[25]  G. Girolami,et al.  Titanium, zirconium, and hafnium tetrahydroborates as "tailored" CVD precursors for metal diboride thin films , 1988 .

[26]  E. Fitzer The future of carbon-carbon composites , 1987 .

[27]  D. Mckee Oxidation behavior and protection of carbon/carbon composites , 1987 .

[28]  H. C. Graham,et al.  Thermogravi metric Study of the Oxidation of ZrB2 in the Temperature Range of 800° to 1500°C , 1971 .